首页> 外国专利> ADDITION METHOD OF POLYMER FOR IMPROVING PARTICLE SHAPE AND DISPERSION STABILITY OF PRECIPITATED CALCIUM CARBONATE BY ADDING PMAA(POLYMETHACRYLIC ACID) OR POLYOXYETHYLENE

ADDITION METHOD OF POLYMER FOR IMPROVING PARTICLE SHAPE AND DISPERSION STABILITY OF PRECIPITATED CALCIUM CARBONATE BY ADDING PMAA(POLYMETHACRYLIC ACID) OR POLYOXYETHYLENE

机译:通过添加PMAA(聚甲基丙烯酸)或聚氧乙烯来改善颗粒状碳酸钙的形状和分散稳定性的聚合物添加方法

摘要

PURPOSE: A method for adding a polymer to a precipitated calcium carbonate suspension is provided, to improve the particle shape and dispersion stability of a precipitated calcium carbonate by adding a polymer surfactant during the electrical conductivity change period in the preparation process of precipitated calcium carbonate. CONSTITUTION: The method comprises the steps of adding a polymer surfactant to a calcium carbonate suspension when the calcium carbonate suspension is prepared by injecting a CO2 gas with stirring at a room temperature, to allow the polymer surfactant to be adsorbed to the surface of the precipitated carbon carbonate; and analyzing the dispersion stability of the precipitated calcium carbonate after filtering and drying. Preferably the CO2 gas is injected with a flow rate of 500 L/min and the suspension is stirred with a velocity of 300 rpm at 20 deg.C to prepare a 3.5 wt% precipitated calcium carbonate suspension. Preferably the polymer surfactant is polyoxyethylene nonylphenyl ether and is added before the carbonation of precipitated calcium carbonate or during the first increase period of electrical conductivity in carbonation, or the polymer surfactant is PMAA(polymethacrylic acid) and is added during the first increase period of electrical conductivity in carbonation.
机译:目的:提供一种将聚合物添加到沉淀碳酸钙悬浮液中的方法,以通过在沉淀碳酸钙的制备过程中在电导率变化期间添加聚合物表面活性剂来改善沉淀碳酸钙的颗粒形状和分散稳定性。组成:该方法包括以下步骤:在室温搅拌下通过注入二氧化碳气体制备碳酸钙悬浮液时,将聚合物表面活性剂添加到碳酸钙悬浮液中,以使聚合物表面活性剂吸附到沉淀的表面上碳酸碳过滤干燥后,析出的碳酸钙的分散稳定性。优选地,以500L / min的流速注入CO 2气体,并且在20℃下以300rpm的速度搅拌该悬浮液以制备3.5wt%的沉淀碳酸钙悬浮液。优选地,聚合物表面活性剂是聚氧乙烯壬基苯基醚,并且在沉淀碳酸钙的碳酸化之前或在碳酸化中的电导率的第一增加期间添加,或者聚合物表面活性剂是PMAA(聚甲基丙烯酸),并且在电学的第一增加期间添加。碳化中的电导率。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号