PURPOSE: Provided are an amorphous perfluorinated homopolymer or copolymer which has a high glass transition temperature (Tg), a specific range of intrinsic viscosity and excellent mechanical properties, and its preparation method and its use for preparing a coating, a film or a layer. CONSTITUTION: The amorphous perfluorinated homopolymer or copolymer comprises 95 mol% or more of a perfluorodioxol represented by the formula IA, wherein R'_F is R_F or OR_F; R_F is a C1-C5 linear or branched perfluoroalkyl radical; and X1 and X2 are identical or different each other and are F or CF3. The amorphous perfluorinated homopolymer or copolymer has a Tg of 180-195 deg.C when measured according to ASTM 3418(DSC) and an intrinsic viscosity of 13-100 cc/g at 30 deg.C when measured in perfluoroheptane according to ASTM D 2857-87.
机译:目的:提供具有高玻璃化转变温度(Tg),特定范围的特性粘度和优异的机械性能的无定形全氟化均聚物或共聚物,其制备方法及其在制备涂层,膜或层中的用途。组成:无定形全氟均聚物或共聚物包含95 mol%或更多的由式IA表示的全氟二恶醇,其中R'_F为R_F或OR_F; R_F是C1-C5直链或支链的全氟烷基。 X1和X2彼此相同或不同,并且为F或CF3。当根据ASTM 3418(DSC)测量时,无定形全氟均聚物或共聚物的Tg为180-195℃,当根据ASTM D 2857在全氟庚烷中测量时,在30℃时的特性粘度为13-100 cc / g。 -87。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号