FIELD: refractory materials.;SUBSTANCE: invention, in particular, relates to linings of metallurgical assemblies, for example coking plants, heating wells, steel-pouring and cast iron-transporting ladles. Invention provides mix comprising quartzite filler, ferrochrome slag, and liquid glass contains, as quartzite filler, waste from production of crystalline quartzites with structure characterized by grain size 0.005-0.05 mm and composed of 7-10% chalcedony, 1-3% accessory minerals, and quartz. Liquid glass with density 1.32 g/cm3 is prepared by direct dissolution, in sodium hydroxide, of waste originating from dry gas-treatment in production of high-percentage ferrosilicium, in particular silicon-containing dust with particle size (50-2500)·10-6 m and content of total carbon 0.3-2.9%, followed by hydrothermal treatment for 60-90 min. Dissolution is carried out at 90-95оС and solid substance-to-liquid weight ratio 1:(1.1-1.6). Percentages of components are the following: above-indicated waste 94-97%, ferrochrome slag 3-6%, and liquid glass 8-14% above 100%.;EFFECT: improved quality of refractories, utilized industrial slag, and widened resource of raw materials for manufacture of refractories at low cost.;5 tbl
机译:技术领域:本发明尤其涉及冶金组件的衬里,例如炼焦厂,加热井,浇铸钢和运输铸铁的钢包。本发明提供了包含石英岩填料,铬铁矿渣和液体玻璃的混合物,其包含作为结晶岩石英石的废料作为石英岩填料,所述结晶石英岩的结构特征在于粒度为0.005-0.05mm,并且由7-10%的玉髓,1-3%的辅助矿物组成。和石英。密度为1.32 g / cm 3 的液态玻璃是通过将氢氧化钠直接溶解于生产高浓度铁硅酸盐中的干燥气体处理产生的废料制成的,特别是含颗粒的含硅粉尘(50-2500)& 10 -6 m,总碳含量为0.3-2.9%,然后进行水热处理60-90分钟。以90-95 ®С进行溶解,固液比为1:(1.1-1.6)。成分百分比如下:上述废料为94-97%,铬铁渣为3-6%,液态玻璃为8-14%(高于100%);效果:提高了耐火材料质量,利用了工业炉渣,拓宽了耐火材料资源。低成本制造耐火材料的原料; 5 tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号