FIELD: chemical technology. SUBSTANCE: invention relates to method for precipitation of different forms of silica from hydrothermal separate that can be used under conditions of geoelectric power plants, geoheating and power plants and in hydrothermal layers. This method can be used for treatment a separate at 20-160 C and pH value from 7.0 to 9.6. Method involves preparing solution supersaturated by amorphous silica, ageing and polymerization with addition of coagulating agents and stirring solution for formation of flakes and precipitation of silica, separation of flakes from cleared solution and preparing flake slime. At the stage of silica precipitation seawater is added to solution with lime simultaneously and seawater must contain total concentration of calcium and magnesium cations from 800 to 1200 mg/kg. Seawater consumption depends on lime consumption and required level of residual concentration of silica in solution after treatment and calcium concentration in precipitated material. Addition of seawater allows reducing lime consumption and to diminish alternation of pH index of solution after treatment with lime. Method provides the possibility to carry out stable precipitation of silica in small consumption of lime and consumption below critical that provides reduction of calcium part in precipitated material to value below 1.0 weight %. EFFECT: improved precipitation method. 1 dwg, 5 tbl, 3 ex
机译:领域:化学技术。发明领域本发明涉及从水热分离物中沉淀不同形式的二氧化硅的方法,该方法可在地热发电厂,地热和发电厂的条件下以及在水热层中使用。该方法可用于分别在20-160℃和pH值为7.0至9.6的条件下进行处理。该方法包括制备被无定形二氧化硅过饱和的溶液,老化和聚合反应,加入凝结剂和搅拌溶液以形成薄片和二氧化硅沉淀,从澄清溶液中分离薄片并制备薄片粘泥。在二氧化硅沉淀阶段,将海水与石灰同时添加到溶液中,海水中钙和镁阳离子的总浓度必须为800至1200 mg / kg。海水消耗量取决于石灰消耗量和处理后溶液中二氧化硅残留浓度的要求水平以及沉淀物质中钙的浓度。添加海水可以减少石灰的消耗,并减少用石灰处理后溶液的pH指数的变化。该方法提供了在少量石灰消耗和低于临界消耗的情况下进行二氧化硅稳定沉淀的可能性,这使得沉淀材料中的钙部分减少到低于1.0重量%的值。效果:改进的沉淀方法。 1桶,5桶,3桶

著录项

  • 公开/公告号RU2219127C2

    专利类型

  • 公开/公告日2003-12-20

    原文格式PDF

  • 申请/专利权人

    申请/专利号RU20020106156

  • 发明设计人 POTAPOV V.V.;POVAROV K.O.;KARPOV G.A.;

    申请日2002-03-06

  • 分类号C01B33/12;C01B33/18;C01B33/24;

  • 国家 RU

  • 入库时间 2022-08-21 22:45:23

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号