Production of cement clinker by preparing raw mixture based on Limestone Saturation Factor, Silica Module and Alumina Module, and fineness adjustment, and controlling conditions at the kiln inlet during clinkering stage

机译:通过基于石灰石饱和因子,二氧化硅模块和氧化铝模块制备原料混合物并调节细度并在熟料阶段控制窑入口的条件来生产水泥熟料

摘要

A cement clinker is produced by preparing a raw mixture based on the Limestone Saturation Factor of up to 1, the Silica Module of 2-3.5 and the Alumina Module of 0-3, and the fineness adjustment in a mesh No. 200 of the raw mixture; and controlling the residence time of the calcinated mixture, clinkering temperature and oxidizing conditions at the kiln inlet during the clinkering stage. Production of a cement clinker involves preheating, calcining, sintering, and cooling a raw mixture. The raw mixture is prepared before the feeding stage based on the Limestone Saturation Factor (LSF) of up to 1, the Silica Module (SM) of 2-3.5 and the Alumina Module (AM) of 0-3, and the fineness adjustment in a mesh No. 200 of the raw mixture to reduce the temperature in the clinkering stage by more than 100 degreesC. The residence time of the calcinated mixture, clinkering temperature and oxidizing conditions are controlled at the kiln (22) inlet during the clinkering stage.
机译:水泥熟料是根据石灰石饱和系数最大为1,二氧化硅模数为2-3.5和氧化铝模数为0-3以及在生料的目号为200的细度调​​节中制备生料混合物而制成的混合物;在熟料阶段控制煅烧混合物的停留时间,熟料温度和窑入口处的氧化条件。水泥熟料的生产涉及预热,煅烧,烧结和冷却原料混合物。原料混合物在进料阶段之前根据最大为1的石灰石饱和因数(LSF),2-3.5的二氧化硅模数(SM)和0-3的氧化铝模数(AM)进行制备,并根据将200目粗混合料降低熟料阶段的温度超过100摄氏度。在熟料阶段,在窑(22)的入口处控制煅烧混合物的停留时间,熟料温度和氧化条件。

著录项

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号