The preparation of glass fibre granules is carried out by mixing cut glass fibres, sized using a size comprising an organosilane, in the presence of 10 to 25 % water for a sufficient time such that the density increases by at least 67 % using a single mixing device which mixes the fibres or granules constantly at the same frequency. The preparation of glass fibre granules is carried out by mixing cut glass fibres, sized using a size comprising an organosilane, in the presence of 10 to 25 % water for a sufficient time such that the density increases by at least 67 % using a single mixing device which mixes the fibres or granules constantly at the same frequency. After drying, the final granules formed contain at least 95 wt.- % glass. A tackifying agent is in contact with the glass fibres at the latest during the mixing. Independent claims are also included for: (a) Glass fibre granules, with a diameter of between 1 and 10 mm and comprising 50,000 to 500,000 glass filaments, obtained by this method; (b) utilization of these granules for reinforcing a thermoplastic.
机译:玻璃纤维颗粒的制备是通过在10%至25%的水存在下将切割的玻璃纤维混合而成的,该切割的玻璃纤维使用包括有机硅烷的胶料进行胶料处理足够的时间,以使一次混合后密度至少增加67%以相同的频率不断混合纤维或颗粒的装置。玻璃纤维颗粒的制备是通过在10%至25%的水存在下将切割的玻璃纤维混合而成的,该切割的玻璃纤维使用包括有机硅烷的胶料进行胶料处理足够的时间,以使一次混合后密度至少增加67%以相同的频率不断混合纤维或颗粒的装置。干燥后,形成的最终颗粒包含至少95重量%的玻璃。增粘剂最迟在混合过程中与玻璃纤维接触。还包括以下方面的独立权利要求:(a)通过该方法获得的直径在1mm至10mm之间并且包含50,000至500,000条玻璃丝的玻璃纤维颗粒; (b)利用这些颗粒增强热塑性塑料。

著录项

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号