首页> 外国专利> Brown oxide pretreatment composition for cleaning copper surface and improving adhesion of polyimide surface, and method for improving adhesion of polyimide surface by applying the same to brown oxide process

Brown oxide pretreatment composition for cleaning copper surface and improving adhesion of polyimide surface, and method for improving adhesion of polyimide surface by applying the same to brown oxide process

机译:用于清洁铜表面并改善聚酰亚胺表面的粘附力的棕色氧化物预处理组合物,以及通过将其应用于氧化棕色方法来改善聚酰亚胺表面的粘附力的方法

摘要

Disclosed herein are a brown oxide pretreatment composition for cleaning a copper surface and improving adhesion of a polyimide surface, and a method for improving adhesion of a polyimide surface by applying the composition to a brown oxide process. The brown oxide pretreatment composition for cleaning a copper surface and improving adhesion of a polyimide surface comprises, 5˜15 g/L of an amine; 190˜210 g/L of a hydroxide compound; at least one additive selected from 3˜6 g/L of a cleaner adjuvant, 0.1˜5 g/L of a antifoaming agent and 1˜10 g/L of a precipitation inhibitor; and the balance of water. When the brown oxide pretreatment composition for cleaning a copper surface and improving adhesion of a polyimide surface is applied to a pretreatment step of a brown oxide process, it can clean a copper surface and improve adhesion of a polyimide surface.
机译:本文公开了用于清洁铜表面并改善聚酰亚胺表面的粘附力的棕色氧化物预处理组合物,以及通过将该组合物应用于棕色氧化物方法来改善聚酰亚胺表面的粘附力的方法。用于清洁铜表面并改善聚酰亚胺表面的粘附力的棕色氧化物预处理组合物包含5〜15g / L的胺; 190〜210g / L的氢氧化物;选自3〜6g / L的清洁助剂,0.1〜5g / L的消泡剂和1〜10g / L的沉淀抑制剂中的至少一种添加剂;和水的平衡。当将用于清洁铜表面并改善聚酰亚胺表面的粘附力的棕色氧化物预处理组合物应用于棕色氧化物工艺的预处理步骤时,它可以清洁铜表面并改善聚酰亚胺表面的粘附力。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号