首页> 外国专利> PROCESS FOR THE MELT SPINNING OF POLYESTER MICROFILAMENTS WITH A DTY TIIRE OF NOT MORE THAN 0 .7 DTEX AND POLYESTER MICROFILAMENTS MANUFACTURED BY THE SAID METHOD

PROCESS FOR THE MELT SPINNING OF POLYESTER MICROFILAMENTS WITH A DTY TIIRE OF NOT MORE THAN 0 .7 DTEX AND POLYESTER MICROFILAMENTS MANUFACTURED BY THE SAID METHOD

机译:干度不超过0 .7 DTEX的聚酯微丝熔融纺丝的工艺及采用SAID方法制造的聚酯微丝熔融纺丝的工艺

摘要

Process for the melt spinning of polyester microfilaments with a DTY titre of not more than 0.7 dtex, characterised in that the microfilaments are spun from the melt of a polyester with reduced relative solution viscosity compared with polyester fibre spinning grades with relative solution viscosities of between 1.60 and 1.65 as a function of their titre, wherein the polyester melt is polyethylene terephthalate and the spinning speed is 2500 m/min ± 10%. The polyester microfilament manufactured by the process have a dyeing uniformity value according to grey scale from 4.0 to 5.0 and a delta E value of less than 1.0.
机译:DTY滴度不超过0.7 dtex的聚酯微丝的熔融纺丝方法,其特征在于,与相对纤维粘度为1.60之间的聚酯纤维纺丝等级相比,微丝从聚酯熔体中纺出,相对溶液粘度降低。 1.65是其滴定度的函数,其中聚酯熔体是聚对苯二甲酸乙二醇酯,纺丝速度是2500m / min±10%。通过该方法制造的聚酯微丝具有根据灰度的从4.0至5.0的染色均匀度值和小于1.0的ΔE值。

著录项

  • 公开/公告号IN2005KN00100A

    专利类型

  • 公开/公告日2005-11-04

    原文格式PDF

  • 申请/专利权人

    申请/专利号IN100/KOLNP/2005

  • 发明设计人 KEMP ULRICH;STIBAL WERNER;

    申请日2005-01-28

  • 分类号D01F6/62;

  • 国家 IN

  • 入库时间 2022-08-21 22:17:36