Disclosed is a process for the deacetylation of chitin and a process for the treatment of chitinaceous materials to obtain chitin which processes are conducted in a non-saponifiable, non-aqueous, water insoluble liquid having a flash point greater than about 100°C, preferably a non-aromatic hydrocarbon. The process for the deacetylation of chitin comprises suspending chitin in the hydrocarbon liquid, preferably from about 0.02 g/cc to about 0.2 g/cc, mixing therewith an alkali metal hydroxide solution, and heating the suspension at a temperature at least about 70°C for a period of time sufficient to obtain the desired degree of deacetylation. The concentration of alkali metal hydroxide in the alkali metal hydroxide solution is at least 30% by weight, preferably at least 40% by weight, and most preferably at least 50% by weight, and the quantity of alkali metal hydroxide is sufficient to provide an alkali metal hydroxide to chitin weight ratio from about (0.35)(AMHMW) / 40 to about (2.5)(AMHMW) / , 40 where AMHMW is the molecular weight of the alkali metal hydroxide.
机译:公开了几丁质脱乙酰基的方法和几丁质材料的处理以获得几丁质的方法,该方法在闪点大于约100℃的非皂化,非水,水不溶性液体中进行,优选非芳香烃。几丁质去乙酰化的方法包括将几丁质悬浮在烃类液体中,优选约0.02g / cc至约0.2g / cc,将其与碱金属氢氧化物溶液混合,并在至少约70℃的温度下加热该悬浮液。持续足以获得所需脱乙酰度的时间。碱金属氢氧化物溶液中碱金属氢氧化物的浓度为至少30重量%,优选至少40重量%,最优选至少50重量%,并且碱金属氢氧化物的量足以提供碱金属氢氧化物与几丁质的重量比为约(0.35)(AMHMW)/ 40至约(2.5)(AMHMW)/ 40,其中AMHMW是碱金属氢氧化物的分子量。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号