LOW CARBON STEEL MANUFACTURING METHOD FOR SECURING CLEANLINESS OF MOLTEN STEEL BY ADDING DEOXIDIZER TO MOLTEN STEEL

机译:通过将脱氧剂添加到熔融钢中来确保熔融钢的洁净度的低碳钢制造方法

摘要

PURPOSE: To provide a manufacturing method of low carbon steel, the method capable of reducing generation of nonmetal inclusions, shortening refining time and improving quality of molten steel through flotation of the nonmetal inclusions in molten steel by adding aluminum as a deoxidizer to molten steel in a process of refining molten steel in converter. CONSTITUTION: The manufacturing method of low carbon steel comprises the steps of performing soft deoxidation by injecting 200 to 350 kg of Al into a converter containing molten low carbon steel comprising 150 to 500 ppm of carbon and 0.020 to 0.050 wt.% of aluminum when content of terminal oxygen is 300 to 700 ppm in the steelmaking process; and manufacturing the low carbon steel by injecting 60 to 200 kg of Al into the soft deoxidation performed molten steel when content of oxygen before deoxidation is 1 to 150 ppm in the RH process and performing reflux operation on the Al injected molten steel for 1 to 7 minutes.
机译:目的:提供一种低碳钢的制造方法,该方法能够通过向钢水中添加铝作为脱氧剂来浮选钢水中的非金属夹杂物,从而减少非金属夹杂物的产生,缩短精炼时间并提高钢水的质量。转炉中精炼钢水的过程。组成:低碳钢的制造方法包括以下步骤:通过将200至350 kg的铝注入到含有熔融低碳钢的转炉中进行软脱氧,该转炉含有150至500 ppm的碳和含量为0.020至0.050 wt%的铝炼钢过程中最终氧的百分数为300至700 ppm;在RH工序中,在脱氧前的氧含量为1〜150ppm的情况下,通过向软质脱氧钢水中注入60〜200kg的Al,并对该Al注入钢水进行1〜7的回流操作,来制造低碳钢。分钟。

著录项

  • 公开/公告号KR20050002323A

    专利类型

  • 公开/公告日2005-01-07

    原文格式PDF

  • 申请/专利权人 POSCO;

    申请/专利号KR20030043696

  • 发明设计人 KWON KI HOON;LEE YOUN WOO;KIM JAE YOUL;

    申请日2003-06-30

  • 分类号C21C7/10;

  • 国家 KR

  • 入库时间 2022-08-21 22:06:04

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号