Provided are incombustible composition excellent in strength, water resistance and processability by using waste materials, and incombustible fire door and wall using the composition by hot pressing. The incombustible composition for fire door(wall) composition comprises the components of: 1-80wt.% of organic fiber such as crushed paper and wood, waste fiber or rice hull, or inorganic fiber such as glass wool or ceramic wool; 1-80wt.% of fly ash or bottom ash; 1-80wt.% of flame retardant such as CaCO3 or NaHCO3; 1-30wt.% of incombustible resin for hardening such as phenolic resin or polyester resin; 1-40wt.% of hollow sphere-type of filler such as perlite, fly ash or ceramics; and optionally 1-50wt.% of weight-lightening material such as perlite or vermiculite, and/or at least one additive selected from hardening promoter(MgO, gypsum plaster), surfactant and inorganic colorant. The incombustible fire door(wall) is manufactured by the following steps of: mixing fly or bottom ash, flame retardant, and resin; adding organic or inorganic fiber to mixtures and mixing, and adding hollow spheres by using air to prevent fibers from agglomerating; hot-pressing mixtures into a plate and/or square bar shape; forming a frame of fire door(wall) with plate and/or square bar, and filling the inside of the frame with fillers such as lightweight foam concrete, lightweight foam mineral board, rock wool, etc.
机译:通过使用废料提供强度,耐水性和加工性优异的不燃组合物,以及通过热压使用该组合物的不燃防火门和墙。防火门(墙)组合物的不可燃组合物包括以下成分:1-80wt。%的有机纤维,如碎纸和木材,废纤维或稻壳,或无机纤维,如玻璃棉或陶瓷棉;粉煤灰或底灰的1-80wt。%; 1-80wt。%的阻燃剂,例如CaCO3或NaHCO3; 1-30wt。%用于固化的不燃树脂,例如酚醛树脂或聚酯树脂; 1-40wt。%的空心球型填料,例如珍珠岩,粉煤灰或陶瓷;和任选地1-50wt。%的减重材料,例如珍珠岩或ver石,和/或至少一种选自硬化促进剂(MgO,石膏灰泥),表面活性剂和无机着色剂的添加剂。不可燃防火门(墙)通过以下步骤制造:将粉煤灰或底灰,阻燃剂和树脂混合;将有机或无机纤维添加到混合物中并混合,并通过使用空气添加空心球以防止纤维团聚;将混合物热压成板和/或方棒状;用板和/或方棒形成防火门(墙)框架,并用轻质泡沫混凝土,轻质泡沫矿物板,岩棉等填充物填充框架的内部。

著录项

  • 公开/公告号KR20050031197A

    专利类型

  • 公开/公告日2005-04-06

    原文格式PDF

  • 申请/专利权人 CHOI JUN HAN;

    申请/专利号KR20030067418

  • 发明设计人 CHOI JUN HAN;LEE SANG HOON;YOON BYUNG ICK;

    申请日2003-09-29

  • 分类号C04B22/10;

  • 国家 KR

  • 入库时间 2022-08-21 22:05:37

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号