The invention of the molten steel upper tapped after the injection of oxygen and Ar gases at a AOD (Argon Oxygen De carburization) refining to remove the C, N, and lowering the oxygen of the molten steel casting ladle in the manufacture of ferritic stainless steel for exhaust after removal of the slag by controlling the molten steel oxygen using a ladle treatment process to improve the cast equiaxed jeongyul relates to a method of improving the cast structure.; The present invention provides a ferritic stainless steel for producing through the AOD refining process and the main jorae the treatment step (LT) for the molten metal melted in an electric furnace to this, the final component added to Ti in the main jorae treatment step (LT) the Cr: 10.0 ~ 12wt%, C: 0.02wt% or less, N: 0.015wt% or less, Si: 0.3 ~ 0.7wt%, S: 0.01wt% or less, Ti: 0.1-0.3wt%, and the balance of Fe and unavoidable It provides a polygonal jeongyul the improved ferritic stainless steel production process consisting of impurities.
机译:在AOD(精炼脱氧剂)精炼过程中注入氧气和Ar气体后精炼钢水的发明,以去除C,N并降低钢水浇铸钢包中的氧气。通过使用钢水包处理工艺来控制钢水氧气以除去铸渣后的排气以改善铸件等轴空浇渣的方法,涉及一种改善铸件结构的方法。本发明提供了一种铁素体不锈钢,其通过AOD精炼工艺和主炉渣生产用于在电炉中熔融的熔融金属的处理步骤(LT),最终组分在主炉渣处理步骤中添加到Ti中( LT)Cr:10.0〜12wt%,C:0.02wt%以下,N:0.015wt%以下,Si:0.3〜0.7wt%,S:0.01wt%以下,Ti:0.1-0.3wt%,以及铁的余量和不可避免的平衡为多边形的jeongyul提供了一种改进的由杂质组成的铁素体不锈钢生产工艺。

著录项

  • 公开/公告号KR20050093292A

    专利类型

  • 公开/公告日2005-09-23

    原文格式PDF

  • 申请/专利权人 POSCO;

    申请/专利号KR20040018563

  • 申请日2004-03-18

  • 分类号C22C38/18;

  • 国家 KR

  • 入库时间 2022-08-21 22:04:32

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号