Elastic surfacing material, characterized in that it is in the form of flame retardants in amounts of from 0,01 to 40 w -%, based on the total weight of the elastic surfacing material, a a phosphinic acid salt of the formula (i) and / or a diphosphinic acid salt of the formula (ii) and / or polymers thereof whereinR1, R2 the same or different and are c1-C.6-Alkyl, linear or branched and / or aryl;R3 C.1-C.10-Alkylene, linear or branched, c.6-C.10-Arylene, - alkyl arylene or - aryl alkylene;M mg, ca, al, sb, sn, ge, ti, zn, fe, zr, ce, bi, sr, mn, li, na and / or k;m 1 to 4;n is 1 to 4;x 1 to 4contains, wherein the elastic surfacing material in order, linoleum, polyvinyl chloride, rubber - rubber - combinations, cork or polymers based on polyurethane and / or styrene - butadiene - latex - base is.
机译:弹性饰面材料,其特征在于,其以阻燃剂的形式存在,基于弹性饰面材料的总重量为0.01至40重量%,式(i)的次膦酸盐和/或式(ii)的二膦酸盐和/或其聚合物,其中R 1 ,R 2 相同或不同且为c 1 -C。 6 -直链或支链和/或芳基的烷基; R 3 C. 1 -C。 10 < / Sub>-直链或支链的亚烷基,c。 6 -C。 10 -亚芳基,-烷基亚芳基或-芳基亚烷基; M mg,ca,al,sb ,sn,ge,ti,zn,fe,zr,ce,bi,sr,mn,li,na和/或k; m 1至4; n为1至4; x 1至4包含,其中弹性堆焊材料按顺序,油毡,聚氯乙烯,橡胶-橡胶-组合,基于聚氨酯和/或苯乙烯-丁二烯-乳胶-基的软木或聚合物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号