PURPOSE: To easily and stably perform the subject processes by carrying out a specific reaction in a mixed system consisting of a vaterite-type calcium carbonate used as a base material, methanol, water and quick lime and/or slaked lime. ;CONSTITUTION: The control of form and the growth of particle of a vaterite-type calcium carbonate having the form defined by formula (DS1 is average particle diameter μm of the major axis of the primary particles measured by a scanning electron microscope) can be performed by charging (A) a carbonation reaction system with (B) water corresponding to 0.1-80 times mol based on calcium carbonate and quick lime and/or staked lime existing in the system A in terms of quick lime, charging the system A with (C) 0.1-25wt.% of calcium carbonate and quick lime and/or slaked lime in terms of solid component of quick lime based on methanol existing in the system and passing CO2 gas through the reaction system consisting of a mixture of B and C to control the system to pH 5.6-11.5 and 15-60°C and control the electrical conductance of the system A to 2-1,000μS to perform the carbonation reaction.;COPYRIGHT: (C)1993,JPO&Japio
机译:目的:通过在混合体系中进行特定反应,轻松,稳定地进行主题过程,所述混合体系由以球ate石型碳酸钙为基础材料,甲醇,水和生石灰和/或熟石灰组成。 ;组成:可以控制具有由式(DS1是通过扫描电子显微镜测量的一次粒子的主轴的平均粒径μm)的形式定义的球ate石型碳酸钙的形式和粒子的生长。通过向碳酸化反应体系中加入(B)相当于碳酸钙和生石灰和/或存在于系统A中的生石灰的0.1-80倍摩尔的水来进行碳酸化反应系统的装料,对系统A进行装料(C)以系统中存在的甲醇为基础的生石灰的固体成分计,碳酸钙和生石灰和/或熟石灰的含量为0.1-25wt。%,并使CO 2 气体通过反应由B和C的混合物组成的系统,以将系统的pH值控制在5.6-11.5和15-60°C并将系统A的电导率控制在2-1,000μS以进行碳酸化反应。 C)1993,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号