A description is given of electrosterically stabilized polyurethane resins having an improved profile of properties, obtainable by a) preparing a hydrophilic and solvent-free macromonomer (A)(ii) with monomodal molecular mass distribution, by a1)reacting 50 to 100 parts by weight of a hydrophilic alkyl- or arylpolyalkylene glycol (A)(i) with 1 to 100 parts by weight of a polyisocyanate component (B)(i) optionally in the presence of a catalyst in the absence of solvents, and subsequently a2) reacting the uniform preadduct from stage a1) completely with 0.5 to 200 parts by weight of a compound (C) in the absence of solvents, and b) by preparing the polyurethane dispersion, by b1)reacting 2 to 50 parts by weight of the hydrophilic and solvent-free macromonomer (A)(ii) with 25 to 250 parts by weight of the polyisocyanate component (B)(i), optionally in the presence of 0 to 50 parts by weight of a solvent component (D) and also of a catalyst, b2) reacting the polyurethane preadduct from stage b1) with 50 to 100 parts by weight of a polymeric polyol (A)(iii) and optionally with 0.5 to 10 parts by weight of a low molecular mass polyol component (A)(iv), optionally in the presence of a catalyst, b3)reacting the homogeneous polyurethane preadduct from stage b2) with 2 to 20 parts by weight of a polyol component (A)(v), optionally in the presence of a catalyst, b4) admixing the homogeneous polyurethane prepolymer from stage b3), before or during dispersion in 50 to 1500 parts by weight of water, with 2 to 20 parts by weight of a neutralizing component (E), b5)dispersing the optionally (partially) neutralized polyurethane prepolymer from stage b4) in 50 to 1500 parts by weight of water, which optionally further contains 0 to 100 parts by weight of a formulating component (F), and finally b6)reacting the (partially) neutralized polyurethane prepolymer dispersion from stage b5) with 3 to 60 parts by weight of a chain extender component (G) and also, subsequently or simultaneously, with 0 to 30 parts by weight of a chain stopper component (H). The performance properties of the polyurethane dispersions of the invention in terms of absence of solvent, and also material properties, are excellent. Also deserving of emphasis are the simplicity and reproducibility of the process and the storage stability of the products.
机译:给出了具有改善的性能曲线的电立体稳定的聚氨酯树脂的描述,该树脂可通过以下方法获得:a)通过制备具有单峰分子量分布的亲水性和无溶剂的大分子单体(A)(ii), a 1 )反应50到100份重量的亲水性烷基或芳基聚亚烷基二醇(A)(i)和1至100重量份的多异氰酸酯组分(B)(i),视情况在催化剂的存在下,在无溶剂的情况下,随后 a 2 )使0.5至200重量份的a 1 )阶段的均匀预加合物完全反应(C)在没有溶剂的情况下制备化合物(C),以及b)通过 b 1 制备聚氨酯分散体2至50重量份的亲水性和无溶剂大分子单体(A)(ii)与25至250重量份的多异氰酸酯组分( B)(i),任选在0至50重量份的溶剂组分(D)以及催化剂的存在下 b 2 )使阶段b 1 )中的聚氨酯预加合物与50至100重量份的聚合多元醇(A)(iii)和可选地与0.5至10重量份的多元醇反应低分子量多元醇组分(A)(iv)的重量,可选地在催化剂存在下 b 3 )将b 2 )阶段的均相聚氨酯预加合物与2至20重量份的多元醇组分(A)(v)反应,可选地在催化剂 < ListItem id =“ ul0003-0006” number =“ 0000”> b 4 )在分散至50至1500之前或之中,将阶段b 3 的均相聚氨酯预聚物进行混合重量份的水和2至20重量份的中和组分(E), b 5 )将来自阶段b 4 的(部分)可选的(部分)中和的聚氨酯预聚物分散在50至1500重量份的水中,该水中还任选包含0到100重量份的配方成分(F),最后 b 6 )进行(部分)中和来自阶段b 5 )的聚氨酯预聚物分散体,其中含有3至60重量份的扩链剂组分(G),并且随后或同时含有0至30重量份的链终止剂组分(G) H)。就不存在溶剂而言,本发明的聚氨酯分散体的性能特性以及材料特性均优异。同样值得强调的是该方法的简单性和可重复性以及产品的储存稳定性。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号