Dimples, preferably 40 to 200 µm in average depthand 0.5 to 3 mm in diameter of circle equivalent, areformed on the peripheral surface of a cooling drum,adjacent to each other at the rims of the dimples; andfine humps (preferably, fine humps 1 to 50 µm in heightand 5 to 200 µm in diameter of circle equivalent on thesurfaces of the dimples and/or fine humps 1 to 50 µm inheight and 30 to 200 µm in diameter of circle equivalentat the rims of the dimples), fine holes (preferably, fineholes 5 µm or more in depth and 10 to 200 µm in diameterof circle equivalent), or fine unevenness (preferably,fine unevenness 1 to 50 µm in average depth and 10 to 200µm in diameter of circle equivalent) are formed at therims and/or on the indented surfaces of said dimples.
机译:凹痕,平均深度优选为40至200 µm等效直径为0.5到3毫米形成在冷却鼓的外围表面上,在酒窝的边缘处彼此相邻;和细小驼峰(最好是高度为1至50 µm的细小驼峰)直径相当于5到200 µm的圆凹坑和/或细小驼峰的表面1至50 µm高度,直径等效为30至200 µm在酒窝的边缘),细孔(最好是细孔)深度为5 µm或更大,直径为10至200 µm的孔或当量的不均匀度(最好是细微的不均匀度,平均深度为1至50 µm,平均深度为10至200在边缘和/或在所述凹坑的凹入表面上。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号