The aim of the invention is to be able to economically use ore dust which is created by the extraction and preparation of iron ore and has not been usable until now. To this end, the invention relates to an agglomerated stone comprising (in wt. %) between 6 and 15 % of a cement binding agent, up to 20 % of a carbon carrier, up to 20 % of residual and recyclable substances, and optionally up to 10 % of an accelerator, the remainder consisting of iron ore in a stone format in the form of particles having a particle size of less than 3 mm. After three days, the iron ore has an initial strength of at least 5 N/mm2, and after 28 days, a cold compression strength of at least 20 N/mm2. As a result of the particular hardness St and form stability thereof even at high temperatures T, inventive agglomerated stones are especially suitable for using in shaft furnaces, corex furnaces, or blast furnaces. The invention also relates to a method for producing inventive agglomerated stones.
机译:本发明的目的是能够经济地使用由铁矿石的提取和制备产生的并且至今尚未使用的粉尘。为此,本发明涉及一种附聚石,其包含(以重量%计)6至15%的水泥粘合剂,至多20%的碳载体,至多20%的残余和可循环利用的物质,以及任选地最多可使用10%的促进剂,其余部分由铁矿石组成,呈铁矿石状,其颗粒形式小于3毫米。三天后,铁矿石的初始强度至少为5 N / mm2,28天后,冷压缩强度为至少20 N / mm2。由于特定的硬度St及其即使在高温T下的形状稳定性,本发明的结石特别适用于竖炉,型芯炉或高炉。本发明还涉及一种生产本发明的结块石的方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号