The present invention is for coating porcelain and it relates to a coating composition and the coating method, to solve The technical challenge is no stain, and a crack for improved wetting and drying rate of the sol is used to form a coating film. ; aspect of the solution according to the invention for this purpose is a solution-based sol, is added to improve the wettability increases the viscosity of the sol dispersing agent, is added comprises acetone and methanol to increase the drying rate of the sol coating composition is disclosed. ; In addition, the present invention A method for forming a coating film is immersed in a ceramic coating composition described above is another aspect of the method according to the resolution, is at least one time in the dipping and drying process of the ceramic coating composition to increase the thickness of the coating film repeating the steps of immersing and drying, temperature 300-600 , time 50 to 70 minutes in a reducing atmosphere of N2 gas, CO gas, this is a coating method comprising the step of heat treatment while flowing a mixed gas of CO2 gas for the heat treatment is started .
机译:本发明涉及涂料的涂覆,涉及涂料组合物和涂覆方法,以解决技术难题是不沾污,并且使用用于改善溶胶的湿润和干燥速率的裂缝来形成涂膜。 ;为此目的,本发明溶液的一个方面是基于溶液的溶胶,被添加以提高润湿性,增加溶胶分散剂的粘度,被添加包含丙酮和甲醇以增加溶胶涂料组合物的干燥速率。披露。 ;另外,本发明的用于形成涂膜的方法被浸入上述陶瓷涂料组合物中,该方法的另一方面是根据分辨率,是在陶瓷涂料组合物的浸渍和干燥过程中至少一次在N2气体,CO气体的还原气氛中,重复浸泡和干燥的步骤(温度300-600,时间50至70分钟),增加涂膜的厚度,这是一种包括以下步骤的涂布方法:开始用于热处理的CO2气体的混合气体。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号