首页> 外国专利> The furniture over-lay fancy plywood manufacture method and the furniture over-lay fancy plywood

The furniture over-lay fancy plywood manufacture method and the furniture over-lay fancy plywood

机译:家具覆面花式胶合板的制造方法及家具覆面花式胶合板

摘要

PURPOSE: Provided are a method for producing an overlay decorative plywood for satinwood, which has excellent gloss, flexibility, lightfastness, water resistance, chemical resistance, and crack resistance and substantially increases life of the satinwood, and an overlay decorative plywood for satinwood produced by the same. CONSTITUTION: The method comprises the steps of (i) applying a urea resin-based adhesive which is a thermosetting resin series, on either side or both sides of panel(10) of high/medium/low density compressed wood such as MDF(medium density fiber), HDF(high density fiber), or general plywood panel(10), so as to form an adhesive layer(11); (ii) impregnating the adhesive layer(11) with UREA-based resin of 7-8 g/ft¬2 to laminate a PAPER(20) with printed pattern on the adhesive layer(11), and primarily adhering the adhesive layer(11) and the PAPER(20) with roll press having temperature of 120-140 deg.C and pressure of 14-16 kg/cm¬2; (iii) mixing a melamine-based resin having water resistance, heat resistance, and cold resistance with 3 wt% of silicon-based resin to form a mixture, and applying the mixture on the top of PAPER(20) of first product obtained by the step(ii) with 4-5 g/ft¬2 to form a second product having resin layer(30); and (iv) passing the second product through furnace maintaining a temperature of 100-120 deg.C to temporarily dry the product, and then thermocompressing the product in thermocompressor(2) of 120-140 deg.C and 14-16 kg/cm¬2.
机译:用途:提供了一种用于缎面装饰用胶合板的生产方法,其具有优异的光泽度,柔韧性,耐光性,耐水性,耐化学药品性和抗裂性,并大大提高了缎面木材的使用寿命,并且提供了一种由相同。组成:该方法包括以下步骤:(i)在高/中/低密度压缩木材(如MDF(中)密度纤维),HDF(高密度纤维)或普通胶合板(10),以形成粘合层(11); (ii)用7-8g / ft 2的尿素基树脂浸渍粘合剂层(11),以将具有印刷图案的PAPER(20)层压在粘合剂层(11)上,并且首先粘合粘合剂层(11)。 )和具有辊压机的PAPER(20),辊压机的温度为120-140℃,压力为14-16 kg / cm 2; (iii)将具有耐水性,耐热性和耐寒性的三聚氰胺基树脂与3wt%的硅基树脂混合以形成混合物,并将该混合物涂覆在通过以下方法获得的第一产品的纸(20)的顶部步骤(ii)以4-5g / ft 2形成具有树脂层(30)的第二产物; (iv)使第二种产品通过保持温度为100-120摄氏度的炉子以暂时干燥产品,然后在120-140摄氏度和14-16 kg / cm的热压机(2)中对产品进行热压¬2。

著录项

  • 公开/公告号KR100549696B1

    专利类型

  • 公开/公告日2006-02-07

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20020035355

  • 发明设计人 홍순관;

    申请日2002-06-24

  • 分类号B32B21/06;

  • 国家 KR

  • 入库时间 2022-08-21 21:24:20