GROUND REINFORCING COMPOSITES IN ENVIRONMENTALLY FRIENDLY INORGANIC SYSTEM AND ITS GROUND REINFORCING CONSTRUCTION METHOD THEREOF
GROUND REINFORCING COMPOSITES IN ENVIRONMENTALLY FRIENDLY INORGANIC SYSTEM AND ITS GROUND REINFORCING CONSTRUCTION METHOD THEREOF
展开▼
机译:环保无机无机系统中的地基增强复合材料及其地基增强方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
The present invention relates to an environment-friendly inorganic ground reinforcement composition and a ground reinforcement method using the same, the purpose of which is that the strength of the cured body is very high, long-term durability is superior, compared to the conventional chemical liquid injection method, can achieve both the permanent order and ground reinforcement It is to provide an environmentally friendly inorganic ground reinforcement composition and ground reinforcement method using the same.;The present invention is alumina cement component 10 ~ 35wt%, calcium sulfoaluminate (CSA) component 25 ~ 45wt%, gypsum 10 ~ 30wt%, calcium fluoroaluminate component 5 ~ 20wt%, reactive modifier (RT) 0.3 ~ 5.0wt It consists of%, and is to reinforce the ground by such ground reinforcement composition.;Grout, ground reinforcement, ground reinforcement composition, soft ground, ground reinforcement method
展开▼