Disclosed are a linear low density polyethylene shrink film of a long side chain type prepared by crosslinking a linear low density polyethylene of a short side chain in an extruder, and a method of manufacturing the same. The method for producing the shrink film is selected from the group consisting of (a) 50 to 95 wt% linear low density polyethylene resin, (b) ethylene vinyl acetate copolymer, low density polyethylene, high density polyethylene, and mixtures thereof, based on the total resin component. Mixing 5 to 50% by weight of the synthetic resin substrate with respect to the total resin component, and (c) 0.02 to 0.3 parts by weight of the crosslinking agent with respect to 100 parts by weight of the total resin component; Melting and kneading the mixture of the linear low density polyethylene resin, the synthetic resin substrate, and the crosslinking agent; And molding the melted and kneaded mixture into a film shape.;Linear Low Density, Shrink Film, Synthetic Resin Base, UV Absorber, Crosslinker, Polyethylene
机译:公开了一种通过在挤出机中交联短侧链的线性低密度聚乙烯而制备的长侧链型线性低密度聚乙烯收缩膜及其制造方法。收缩膜的制造方法选自(a)50〜95重量%的线性低密度聚乙烯树脂,(b)乙烯-乙酸乙烯酯共聚物,低密度聚乙烯,高密度聚乙烯及其混合物。总树脂成分。相对于全部树脂成分,混合5〜50重量%的合成树脂基板,相对于100重量份的树脂成分,混合(c)0.02〜0.3重量份的交联剂。将线性低密度聚乙烯树脂,合成树脂基材和交联剂的混合物熔融并捏合;并将熔融和捏合的混合物成型为薄膜状;线性低密度,收缩薄膜,合成树脂基,紫外线吸收剂,交联剂,聚乙烯

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号