just a piece of manufacturing chain (short side chain) in the form of a linear low density polyethylene crosslinked by reacting in the extruder side chain (long side chain) in the form of a linear low density polyethylene shrink film and its manufacturing method are disclosed. A method for fabricating a shrink film with respect to (a) the total resin components, 50 to 95% by weight of linear low density polyethylene resin, (b) an ethylene-vinyl acetate copolymer, selected from low density polyethylene, high density polyethylene, and the group consisting of a mixture of these and, from 5 to 50% by weight relative to the total resin component synthetic resin substrate, and (c) mixing the total resin composition from 0.02 to 0.3 parts by weight of a crosslinking agent based on 100 parts by weight; The linear low-density polyethylene resin, melting the mixture of the synthetic resin substrate and a cross-linking agent, to the kneading step; And the melt, a step of molding the kneaded mixture into a film.
机译:仅公开了通过在线性低密度聚乙烯收缩膜形式的挤出机侧链(长侧链)中反应而交联的线性低密度聚乙烯形式的制造链(短侧链)及其制造方法。相对于(a)全部树脂组分,50至95重量%的线性低密度聚乙烯树脂,(b)选自低密度聚乙烯,高密度聚乙烯的乙烯-乙酸乙烯酯共聚物的收缩膜的制造方法,和由它们的混合物组成,和相对于总树脂组分合成树脂基材为5至50重量%的混合物,和(c)将总树脂组合物为0.02至0.3重量份的交联剂基混合每100重量份;线性低密度聚乙烯树脂,将合成树脂基材和交联剂的混合物熔融,进行捏合步骤;然后是熔融,将捏合的混合物模制成膜。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号