摘要

present invention is plastic waste (PET bottles) and processed polyethylene terephthalate (polyethylen terephthalate: PET) fiber in the material or polypropylene (PP) or polyester (PE) relates to a construction method using the block grid in the field mortar poured slope woven fiber reinforcement in the mold to the material, more particularly fiber reinforced slope mold and four days Soil In construction methods using, to the construction protrusions 41 and the fill material (45) composed of slope reinforcement fiber junction die 43 is not injected (40) is formed by injecting a filler in these time sikyeoteul 45 to surface 1 position and 75 to 80 parts by weight of cement mortar composition with respect to 100 parts by weight of the slope reinforcement fiber die 40 to form the projections 41, the waste plastic (PET bottle), a recycled polyethylene terephthalate to ( polyethylen terephthalate: PET) when cutting the fiber having a thickness of 1.0-2.0mm, and a length of injecting fill material (45) consisting of fiber reinforcement 0.5-2.0 parts by weight of 2-7 and the fill material 45 is fully cured joints (43 ), and the incision is formed in the horizontal direction on the basis of 15 degrees to 20 degrees given the inclined hole 56 to surface 1 through the incision with the joint 43 and fix the Soil nail (55) and the hole ( 56), and grouting with cement mortar in the joints incision that 43 out of Soil nail (55) did not establish the joint (43), and fill the earth and sand after the incision after natural grass, vegetation acids, such as flowers or seeds sown characterized by vegetation.
机译:本发明是在塑料废料(PET瓶)和加工过的聚对苯二甲酸乙二醇酯(聚对苯二甲酸乙二酯:PET)纤维中的材料或聚丙烯(PP)或聚酯(PE)的建筑方法,涉及一种利用块状网格在现场用砂浆浇筑的斜交编织纤维在模具中对材料进行加固,特别是纤维增强的坡口模具和四天土壤在采用的施工方法中,向施工突起41和填充材料(45)组成的坡口不注入纤维结模43(40)是相对于100重量份的斜坡增强纤维模具40,通过在此时将sikyeoteul 45注入填料至表面1位置和75至80重量份水泥砂浆组合物以形成凸起41,废塑料(PET)而形成瓶子),切割厚度为1.0-2.0mm的纤维以及注入填充物的长度时,将回收的聚对苯二甲酸乙二醇酯制成(聚对苯二甲酸乙二酯:PET)由纤维增强材料0.5-2.0重量份的2-7和填充材料45组成的第三层(45)是完全固化的接缝(43),并且在给定的15度到20度的水平方向上形成切口将倾斜的孔56穿过带有接缝43的切口固定到表面1上,并固定土钉(55)和孔(56),并在接缝切口中用水泥砂浆注浆,以确保土钉(55)中的43个没有建立关节(43),并在切口后将天然草,植物酸(例如以植物为特征播种的花朵或种子)填满土和沙。

著录项

  • 公开/公告号KR100632494B1

    专利类型

  • 公开/公告日2006-10-13

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20030098074

  • 发明设计人 최영근;

    申请日2003-12-27

  • 分类号E02D17/20;E02B3/12;A01G1;A01C1;

  • 国家 KR

  • 入库时间 2022-08-21 21:22:52

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号