The method involves five steps for mixing. In the first step (S1) 57 grams of mortar compound is mixed in 1 liter water. In the second step (S2) the mixture is mixed in an empty mixer with 4 liters of water. In the third step (S3) 15 kg cement is mixed for 2 minutes. Step four (S4) involves addition of 85 kg sand. Mixing time should be 5 minutes. In the fifth step (S5) more water is mixed till desired consistency. Independent claims are also included for the following: (A) Mortar compound; and (B) Metering unit.
机译:该方法包括五个混合步骤。在第一步(S1)中,将57克的砂浆混合在1升水中。在第二步(S2)中,将混合物在空混合器中与4升水混合。在第三步骤(S3)中,将15kg水泥混合2分钟。第四步(S4)涉及添加85公斤沙子。混合时间应为5分钟。在第五步骤(S5)中,将更多的水混合直至期望的稠度。还包括以下方面的独立权利要求:(A)砂浆化合物; (B)计量单元。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号