PROBLEM TO BE SOLVED: To provide a high-strength low-alloy steel boiler tube for which heat-treatment is simplified and which is excellent in long-term creep rupture property and high-temperature strength property when used in a high-temperature/high-pressure environment, and a method of manufacturing the same.;SOLUTION: The high-strength low-alloy steel boiler tube for which heat-treatment is simplified comprises, by mass, 0.03-0.15% C, 0.10-0.80% Si, 0.10-1.50% Mn, ≤0.030% P, ≤0.010% S, ≤0.020% O, 0.001-0.01% N, ≤0.01% Al, 0.30-0.80% Cr, ≥0.01% but 0.50% Mo as basic components and the balance being Fe and unavoidable impurities, preferably has a metal structure with a ferrite fraction of 10-90% and is used without any further treatment after normalizing.;COPYRIGHT: (C)2007,JPO&INPIT
机译:要解决的问题:提供一种高强度低合金钢锅炉管,该管简化了热处理,并且在高温/高温下使用时具有长期蠕变断裂特性和高温强度特性优良的特点。解决方案:解决方案:简化了热处理的高强度低合金钢锅炉管的质量百分比为0.03-0.15%C,0.10-0.80%Si,0.10 -1.50%Mn,0.013%P,0.010%S,0.020%O,0.001-0.01%N,0.01%Al,0.30-0.80%Cr,0.01%但Mo <0.50%作为基本成分,其余部分为铁和不可避免的杂质,最好具有铁素体含量为10-90%的金属结构,并且在归一化后无需任何进一步处理即可使用。;版权:(C)2007,JPO&INPIT

著录项

  • 公开/公告号JP2007217783A

    专利类型

  • 公开/公告日2007-08-30

    原文格式PDF

  • 申请/专利权人 NIPPON STEEL CORP;

    申请/专利号JP20060043054

  • 发明设计人 MURAKI TARO;ASAHI HITOSHI;

    申请日2006-02-20

  • 分类号C22C38/00;C22C38/22;C22C38/60;C21D1/28;C21D9/08;

  • 国家 JP

  • 入库时间 2022-08-21 21:14:15

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号