PPROBLEM TO BE SOLVED: To provide a deterioration hysteresis determination method for a light-weight cellular concrete (ALC) capable of determining, totally and in detail, the durability of the ALC that has been used over the years. PSOLUTION: Steam adsorption isotherms in adsorption and desorption are acquired as to one part collected from the ALC, and the levels of hysteresis in the obtained steam adsorption isotherms serve as a deterioration history in the ALC. This method determines that the ALC, of which the hysteresis (1-Wa/Wd) in the steam adsorption isotherm obtained, based on an equilibrium moisture content Wa at 0.6 of the relative pressure in the adsorption, and based on an equilibrium moisture content Wd at 0.6 of the relative pressure in desorption, is 0.1 or larger, as having gone through a moderate deterioration history, and determines that the ALC of which the hysteresis (1-Wa/Wd) to be 0.075 or smaller, as having gone through an abrupt deterioration history. PCOPYRIGHT: (C)2007,JPO&INPIT
机译:

要解决的问题:提供一种用于轻质多孔混凝土(ALC)的劣化滞后测定方法,该方法能够完全详细地确定多年来使用的ALC的耐久性。

解决方案:从ALC中收集了一部分吸附和解吸中的蒸汽吸附等温线,并且所获得的蒸汽吸附等温线中的滞后水平成为ALC中的劣化历史。该方法基于在吸附的相对压力为0.6时的平衡水分含量Wa和吸附水分的平衡水分含量Wd来确定获得了蒸汽吸附等温线的磁滞(1-Wa / Wd)的ALC。在解吸的相对压力为0.6时,如果经历了中等程度的劣化历史,则为0.1或更大,并确定在经过解吸后的滞后(1-Wa / Wd)的ALC为0.075或更小。突然恶化的历史。

版权:(C)2007,日本特许厅&INPIT

著录项

  • 公开/公告号JP2007171125A

    专利类型

  • 公开/公告日2007-07-05

    原文格式PDF

  • 申请/专利权人 SUMITOMO KINZOKU KOZAN SIPOREX KK;

    申请/专利号JP20050372777

  • 发明设计人 MATSUSHITA FUMIAKI;

    申请日2005-12-26

  • 分类号G01N30/00;G01N17/00;G01N15/08;

  • 国家 JP

  • 入库时间 2022-08-21 21:12:01

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号