The steel null carbon content for carburization which is superior

机译:渗碳钢零碳含量优越

摘要

PROBLEM TO BE SOLVED: To improve torsional fatigue characteristics in steel to be carburized.;SOLUTION: In the steel to be carburized, which has a carbon content of 0.1-0.3 mass% and contains Cr, this steel includes at least one element selected among Co, Ni, and Cu, in a range satisfying the expression (1): [Co]+2.1×[Ni]+2.8×[Cu]-2.4×[Cr]0, (where [Co], [Ni], [Cu], or [Cr] indicates respectively Co content in the steel (mass%), Ni content (mass%), Cu content (mass%), or Cr content (mass%)).;COPYRIGHT: (C)2003,JPO
机译:解决的问题:为了改善渗碳钢的扭转疲劳特性;解决方案:在渗碳钢中,碳含量为0.1-0.3质量%,并且含有Cr,该钢包括至少一种选自以下元素: Co,Ni和Cu在满足表达式(1)的范围内:[Co] + 2.1×[Ni] + 2.8×[Cu] -2.4×[Cr]> 0,(其中[Co], [Ni],[Cu]或[Cr]分别表示钢中的Co含量(质量%),Ni含量(质量%),Cu含量(质量%)或Cr含量(质量%))。日本特许厅(C)2003

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号