PROBLEM TO BE SOLVED: To discharge molten slag of low copper grade to the outside of a furnace through a slag discharge hole provided to the outer-end side wall of a settler of the flash smelting furnace without mixing a matte. ;SOLUTION: While blowing, powdery coke for keeping an operating temperature into a shaft 2 provided in a flash smelting furnace 1 and also keeping the layer thickness of molten slag 6 standing within a settler 3 to ≥500 mm, the molten slag 6 is discharged to the outside of the furnace through a slag discharge hole 8 provided, corresponding to the level of the intermediate part of the slag layer thickness in the height direction, to the outer-end side wall of the settler 3. Because the slag discharge is done by discharging the slag from the intermediate layer of low copper grade without discharging the slag from the upper-end and the lower-end layers of high copper grade, among the slag layers, the loss of copper into the slag can be reduced. Further, continuous tapping of the slag can also be performed by setting up the port diameter of the slag discharge hole 8 to 90 to 100 mm.;COPYRIGHT: (C)2000,JPO
机译:解决的问题:通过设置在闪速熔炼炉的沉降器的外端侧壁上的熔渣排放孔将低铜等级的熔渣排放到熔炉的外部,而无需混合毛面。 ;解决方案:在吹炼粉状焦炭的同时,为了保持进入闪速熔炉1中的竖井2中的工作温度,并且还保持位于沉淀器3内的熔渣6的层厚度达到500 mm,该熔渣6为通过设置在炉渣外部的侧壁上的,与炉渣层厚度的中间部分的高度相对应的炉渣排出孔8,将该炉渣排出孔8排出到炉外。通过从低铜等级的中间层排出炉渣而不从高铜等级的上端和下端层排出炉渣,在炉渣层之间,可以减少铜向炉渣中的损失。另外,也可以通过将排渣孔8的端口直径设置为90至100mm来连续排渣。版权所有:(C)2000,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号