摘要

PURPOSE: To produce a thin-walled spheroidal graphite cast iron minimal in the occurrence of chill and also to produce automobile parts by using this material. ;CONSTITUTION: The thin-walled spheroidal graphite cast iron has a composition consisting of, by mass ratio, 3.0-4.0% C, 1.5-2.4% Si, 0.3% Mn, 0.05% P, 0.009-0.016% S, 0.02-0.06% Mg, 5-60ppm Bi, and the balance Fe with inevitable impurities and further has a chilled carbon equivalent (CEc) represented by equation, CEc=C%+αSi%, where 1α≤2 is satisfied. By this method, the sound thin-walled spheroidal graphite cast iron, in which the occurrence of chill in the thin-walled part of ≤3mm thickness in an as-cast state is controlled to ≤2%, can be obtained.;COPYRIGHT: (C)1996,JPO
机译:目的:生产一种薄壁的球墨铸铁,在发生冷风的情况下最少,并使用这种材料生产汽车零件。组成:薄壁球墨铸铁的成分为质量比为3.0-4.0%C,1.5-2.4%Si,<0.3%Mn,<0.05%P,0.009- <0.016%S, 0.02-0.06%Mg,5-60ppm Bi和余量的Fe具有不可避免的杂质,并且还具有等式表示的冷碳当量(CEc),CEc = C%+αSi%,其中1 <α&le; 2很满意。通过这种方法,可以得到声音良好的薄壁球墨铸铁,其中铸态的厚度小于3mm的薄壁部分的发冷控制在2%。版权所有:(C)1996,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号