An aluminum alloy for casting with excellent rigidity and having a low coefficient of linear expansion containing 13-25% by mass of silicon, 2-8% by mass of copper, 0.5-3% by mass of iron, 0.3-3% by mass of manganese, 0.001-0.02% by mass of phosphorus, and the remainder comprising aluminum and inevitable impurities, wherein the total amount of iron and manganese is 3.0% by mass or greater. Said alloy may further contain 0.5-6% by mass of nickel, and the total amount of iron, manganese, and nickel may be 3.0% by mass or greater. Further, said alloy may further contain one or more of 0.1-1.0% by mass of chromium, 0.05-1.5% by mass of magnesium, 0.01-1.0% by mass of titanium, 0.0001-1.0% by mass of boron, 0.1-1.0% by mass of zirconium, 0.1-1.0% by mass of vanadium, or 0.01-1.0% by mass of molybdenum.
机译:具有优异的刚性并且具有低的线性膨胀系数的铸造用铝合金,其包含硅13-25质量%,铜2-8%质量,铁0.5-3%质量,0.3-3%质量锰的含量为0.001-0.02质量%,其余包含铝和不可避免的杂质,其中铁和锰的总量为3.0质量%以上。所述合金可以进一步包含0.5质量%至6质量%的镍,并且铁,锰和镍的总量可以为3.0质量%以上。此外,所述合金可进一步包含0.1-1.0质量%的铬,0.05-1.5质量%的镁,0.01-1.0质量%的钛,0.0001-1.0质量%的硼,0.1-1.0中的一种或多种。按质量百分比计的锆,按质量计0.1%至1.0%的钒或按质量计0.01%至1.0%的钼。

著录项

  • 公开/公告号US2007193663A1

    专利类型

  • 公开/公告日2007-08-23

    原文格式PDF

  • 申请/专利权人 KAZUHIRO ODA;MASAHIKO SHIODA;

    申请/专利号US20050593338

  • 发明设计人 KAZUHIRO ODA;MASAHIKO SHIODA;

    申请日2005-03-23

  • 分类号C22C21/04;

  • 国家 US

  • 入库时间 2022-08-21 21:06:52

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号