摘要

An improved system for comparative evaluation of slag corrosion resistance of different quality of refractories with desired metal and slag chemistry and the system comprises induction furnace (6) having inner volume such that 18 to 20 kg of metal can be melted, plurality of sample specimens (1) of different qualities, definite proportions of slag (5) and metal (4) inside the plurality of sample specimens (1), insulations of definite thickness and means (3) adapted for resisting metal-slag attack. The process for comparative evaluation of slag corrosion resistance of different quality refractories with desired metal and slag chemistry comprises lining of the induction furnace with sample specimens, addition of metal/steel to the induction furnace and heating and melting to attain desired temperature, addition of definite amount of slag of definite composition in the furnace, maintaining desired temperature ranging, draining out of metal and slag after completion of desired duration of evaluation, determining thickness of corroded sample specimens and evaluation of corrosion index.[IN227272A1]
机译:一种改进的系统,用于比较评估具有所需金属和炉渣化学性质的不同耐火材料质量的耐熔渣腐蚀性能,该系统包括感应炉(6),其内部容积可熔化18至20 kg的金属,多个样品样本( 1)具有不同的质量,在多个样品样本(1)内有一定比例的炉渣(5)和金属(4),一定厚度的绝缘材料和适于抵抗金属炉渣侵蚀的装置(3)。比较具有所需金属和炉渣化学性质的不同耐火材料的耐渣腐蚀性能的方法包括:在感应炉中衬上样品,向感应炉中添加金属/钢,加热熔化以达到所需温度,并添加一定量的耐火材料。炉中一定成分的炉渣数量,保持所需的温度范围,在完成所需的评估时间后,将金属和炉渣排出,确定腐蚀样品的厚度并评估腐蚀指数。[IN227272A1]

著录项

  • 公开/公告号IN2005KO00167A

    专利类型

  • 公开/公告日2007-04-06

    原文格式PDF

  • 申请/专利权人

    申请/专利号IN167/KOL/2005

  • 发明设计人

    申请日0000-00-00

  • 分类号

  • 国家 IN

  • 入库时间 2022-08-21 20:58:07

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号