In a method for removing chromium oxide and nickel oxide, and combinations thereof, from liquid slags or slag mixtures, in which the liquid slag is A charged onto a metal bath, in particular an iron bath, and reduced by feeding carbon or carbon carriers, the carbon feed into the metal bath is effected until a decrease of the Cr and/or Ni oxide contents of the slag to a value of between 0.8 wt.-% and 0.2 wt.-%. As the pregiven Cr and/or Ni oxide content range of the slag is reached, reductants having higher reduction potentials such as, e.g., Al, Ca, Si, Fe-Si or Ca-Si are added in order to lower the Cr and/or Ni oxide contents to below 0.15 wt.-%, preferably below 0.08 wt.-%.