METHOD FOR DEVELOPING AN IMPROVED OXIDE COATING AND COMPONENTS MADE OF AUSTENITIC STAINLESS STEEL OR NICKEL ALLOY STEEL

机译:奥氏体不锈钢或镍合金钢制成的改进的氧化物涂层和成分的方法

摘要

A method for creating an oxide coating on the surface of a component formed from austenitic stainless steel or nickel alloy steel is set forth. The component has a naturally formed oxide film at the surface. The naturally formed oxide is enhanced through a process comprising at least two steps. In the first step, the component is heated in the presence of circulating dry air for a first period of time at a temperature of approximately 300 degrees centigrade. In the second step, the component is heated in the presence of static dry air at an elevated pressure for a second period of time at a temperature that is higher than the temperature during the first period. The exterior portion of the enhanced oxide coating is removed with an oxidizing treatment whereby an oxide coating having a high ratio of chromium to iron is exposed at the surface of the stainless steel.
机译:提出了一种在由奥氏体不锈钢或镍合金钢形成的部件的表面上形成氧化物涂层的方法。该部件在表面具有自然形成的氧化膜。天然形成的氧化物通过包括至少两个步骤的方法得到增强。在第一步中,在循环干燥空气的存在下,将组件在大约300摄氏度的温度下加热第一时间。在第二步骤中,在存在静态干燥空气的情况下,在升高的压力下在高于第一时间段的温度的温度下在第二时间段中加热组件。通过氧化处理去除增强的氧化物涂层的外部,由此在不锈钢的表面上暴露出具有高的铬与铁比率的氧化物涂层。

著录项

  • 公开/公告号AT364735T

    专利类型

  • 公开/公告日2007-07-15

    原文格式PDF

  • 申请/专利权人 SEMITOOL INC.;

    申请/专利号AT19990916437T

  • 发明设计人 RAYMOND W.;ARTHUR H.;

    申请日1999-04-07

  • 分类号C23C8/10;C23C8/02;C23C8/14;C23C8/16;C23C8/18;C23C8/80;C23C22/06;C23C22/08;

  • 国家 AT

  • 入库时间 2022-08-21 20:55:05

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号