This invention provides a method for manufacturing an aluminum support for a lithographic printing plate material that, even when the speed of electrochemical surface roughening treatment by web transfer, the electrochemical surface roughening treatment plate width of an aluminum plate, and the current density have been change, can realize an identical surface roughened shape and is small in unevenness in manufacture. There are also provided an aluminum support for a lithographic printing plate material, having excellent printing durability, stain resistance and tone reproduction, a lithographic printing plate material, and a method for image formation. The method for manufacturing an aluminum support for a lithographic printing plate material is characterized in that the electrode construction of a treatment tank for electrochemical surface roughening treatment is such that the number of electrodes (1φ) using a three-phase power supply is at least 3 to 5, the time necessary for passage by web transfer through between the electrodes is 0.15 to 0.60 sec, and the ratio between the time necessary for passage through directly under the electrodes and the time necessary for passage through between the electrodes (directly under the electrodes/between the electrodes) is 1.5 to 3.5.
机译:本发明提供了一种用于平版印刷版材的铝载体的制造方法,该方法即使通过卷筒纸转印进行电化学表面粗糙化处理的速度,铝板的电化学表面粗糙化处理板的宽度和电流密度也发生了变化。 ,可以实现相同的表面粗糙形状,并且制造不均少。还提供了一种用于平版印刷版材的铝载体,其具有优异的印刷耐久性,耐污染性和色调再现性,平版印刷版材以及图像形成方法。用于平版印刷版材的铝载体的制造方法的特征在于,用于电化学表面粗糙化处理的处理槽的电极构造为使得使用三相电源的电极(1φ)的数量至少为3个。参照图5至图5,通过幅材通过电极之间的传递所需的时间为0.15至0.60秒,并且通过电极正下方所需的时间与通过电极之间(电极下方直接)所需的时间之间的比率。 (在电极之间的/)为1.5至3.5。

著录项

  • 公开/公告号WO2007097105A1

    专利类型

  • 公开/公告日2007-08-30

    原文格式PDF

  • 申请/专利号WO2006JP325497

  • 发明设计人 SATO ATSUSHI;

    申请日2006-12-21

  • 分类号B41N3/03;B41N1/14;C25F7/00;G03F7/00;G03F7/004;G03F7/09;

  • 国家 WO

  • 入库时间 2022-08-21 20:48:11

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号