A process is provided for the leaching of both the "limonite" (Fe approx. =25% and Mg approx. =6%) and "saprolite" (Fe approx. =20% and Mg approx. =10%) fractions of typical nickel and cobalt bearing laterite ore. The low magnesium fraction of the laterite ore is leached with sulfuric acid at high pressure and temperature to solubilize the metal values while precipitating most of the solubilized iron as hematite or other iron compounds and a portion of the dissolved aluminum as alunite or other aluminum compounds. After reducing the pressure of the leach slurry to approximately atmospheric pressure, the pregnant leach slurry or solution is contacted with the high magnesium fraction of the ore to solubilize most of the nickel contained in the high-magnesium ore fraction while dissolving only a small portion of the iron content of the high magnesium ore fraction. Further neutralization of the leach slurry in the presence of an alkali metal or ammonium ion will allow the precipitation of iron-bearing jarosite at ambient pressure. This process for incorporating the leaching of saprolite in the high pressure leaching process for limonite ores requires neither high temperature and pressure, nor special treatment of the saprolite ore fraction, nor the addition of special reagents, e.g. reducing reagents.
机译:提供了一种浸出“褐铁矿”(Fe约> = 25%,Mg约> = 6%)和“腐泥土”(Fe约<= 20%,Mg约> = 10%)的工艺。 )典型的含镍和钴的红土矿石的馏分。在高压和高温下,用硫酸浸提低含量红土矿石中的镁,以溶解金属元素,同时使大部分溶解的铁沉淀为赤铁矿或其他铁化合物,而一部分溶解的铝沉淀为白矾石或其他铝化合物。在将浸出浆液的压力降低到大约大气压后,使浸出的浸出浆液或溶液与矿石中的高镁级分接触,以溶解高镁矿石级分中所含的大部分镍,同时仅溶解其中的一小部分。高镁矿石部分的铁含量。在碱金属或铵离子存在下进一步中和浸出浆液将使含铁黄钾铁矾在环境压力下沉淀。在褐铁矿矿石的高压浸出过程中结合腐泥土的这种方法既不需要高温高压,也不需要对腐泥土矿石级分进行特殊处理,也不需要添加特殊的试剂,例如硅藻土。还原剂。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号