A method for refining ultra-low phosphorous steel in a converter, which improves productivity by reducing the steelmaking time of a converter process, can reduce the manufacturing cost of molten steel by reducing the injection quantity of subsidiary raw materials, and can control phosphorous in molten steel stably, is provided. A converter refining method comprises: a step(S10) of charging principal raw materials of hot metal and iron scrap into a converter; a first blowing step(S20) of dephosphorizing the hot metal; a step(S30) of performing a middle discharging process of the dephosphorized slag; and a second blowing step(S40) of decarburizing hot metal from which the slag is discharged, wherein sintered ore is injected into the converter in an amount of 1.7% or more of the total charging amount, or blast furnace return ore is injected into the converter in an amount of 2.6% or more of the total charging amount after performing the step(S10).
机译:一种转炉中超低磷钢的精炼方法,其通过减少转炉过程的炼钢时间来提高生产率,可以通过减少辅助原料的注入量来降低钢水的制造成本,并可以控制熔融金属中的磷提供稳定的钢。转炉精炼方法包括:将铁水和废铁的主要原料装入转炉的步骤(S10)。使铁水脱磷的第一吹制步骤(S20);进行脱磷炉渣的中间排出工序的步骤(S30)。排渣的铁水脱碳的第二吹炼步骤(S40),其中将烧结矿以总装料量的1.7%或更多的量注入转炉,或将高炉回流矿石注入其中。在执行步骤(S10)之后,转换器的充电量为总充电量的2.6%或更多。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号