FIELD: medical devices, namely processes for forming coatings on surfaces of implants made of titanium in recrystallized or nano-structure state.;SUBSTANCE: coating contains, mass %: calcium titanate, 7 - 9; titanium pyrophosphate, 16 - 28; calcium phosphate compounds, the balance. Method comprises steps of anodizing implant by pulse electric current at condition of electric-spark discharge in phosphoric acid solution containing hydroxyapatite and calcium carbonate. Anodizing is realized by means of pulse current with next parameters: pulse time period, 50 - 200 ms; pulse repetition frequency 50 - 100 Hz; initial electric current density, 0.2 - 0.25 A/mm2; final voltage 100 -300 V. Invention allows to receive coating with thickness 40 - 80 micrometers.;EFFECT: possibility for forming coating whose composition is similar to that of osseous tissue with high content of calcium, improved osteoinductive and mechanical properties of coating.;7 cl, 3 ex
机译:领域:医疗器械,即在钛合金制成的再结晶或纳米结构状态的植入物表面上形成涂层的方法。物质:涂层中质量分数为7-9的钛酸钙;焦磷酸钛16-28;磷酸钙化合物,平衡。该方法包括在含有羟磷灰石和碳酸钙的磷酸溶液中在电火花放电条件下通过脉冲电流对植入物进行阳极氧化的步骤。通过具有以下参数的脉冲电流实现阳极氧化:脉冲时间周期:50-200 ms;脉冲重复频率50-100 Hz;初始电流密度0.2-0.25 A / mm 2 ;最终电压为100 -300V。本发明允许接受厚度为40-80微米的涂层。效果:可以形成与钙含量高的骨组织相似的涂层,改善了涂层的骨诱导和机械性能。 7 cl,3 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号