Polyurethane-wood composite, useful for making blocks and boards of high flame resistance, comprises wood particles or fibers and, as binder, isocyanate-containing prepolymer

机译:聚氨酯-木材复合材料,可用于制造高阻燃性的砌块和木板,包含木材颗粒或纤维,以及含异氰酸酯的预聚物作为粘合剂

摘要

Polyurethane-wood composite (A) comprises (a) 50-97.5wt.% wood particles, including fibers (X); (b) 50-2.5wt.% solid, isocyanate-containing prepolymer (PP), based on polyurethane solvolyzate and polyisocyanate; (c) 0-25% other solid additives, including fillers, flame-proofing agents and/or colors; (d) 0-25% other milled polymers, including polyurethanes (PU), polyisocyanurates and/or melamine resins and/or (e) optionally a covering film, on one or both sides of the composite. An independent claim is included for preparing (A) by subjecting a mixture of wood particles and a finely-milled isocyanate-containing oligourethane (produced by polyurethane solvolysis and with 0.5-15wt.% free isocyanate groups), solid at room temperature and containing catalysts, to pressure and temperature for 1-60 minutes.
机译:聚氨酯-木材复合材料(A)包括(a)50-97.5wt。%的木材颗粒,包括纤维(X); (b)50-2.5重量%的固体,含异氰酸酯的预聚物(PP),基于聚氨酯溶剂分解物和多异氰酸酯计; (c)0-25%的其他固体添加剂,包括填料,阻燃剂和/或颜料; (d)在复合材料的一侧或两侧,含0-25%的其他研磨聚合物,包括聚氨酯(PU),聚异氰脲酸酯和/或三聚氰胺树脂和/或(e)可选的覆盖膜。包括一个独立的权利要求,用于制备(A),方法是使木材颗粒和精细研磨的含异氰酸酯的低聚乙烷(通过聚氨酯溶剂分解法生产,具有0.5-15wt%的游离异氰酸酯基)的混合物在室温下为固体,并包含催化剂,在压力和温度下保持1-60分钟。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号