Ni-based alloy with excellent corrosion resistance against supercritical water environment containing inorganic acid

机译:镍基合金,对含无机酸的超临界水环境具有优异的耐腐蚀性

摘要

PPROBLEM TO BE SOLVED: To provide an Ni based alloy which has excellent corrosion resistance to supercritical water containing inorganic acid such as hydrochloric acid caused by the decomposition and oxidation of organic harmful matters such as PCB (polychlorinated biphenyls) and dioxine, and to provide a member for a supercritical water process reaction vessel consisting of the Ni based alloy. PSOLUTION: The Ni based alloy having excellent corrosion resistance to inorganic acid-containing supercritical water environment has a composition containing 29 to 42% Cr, 1 to 3% Ta, 0.001 to 0.05% Mg, 0.001 to 0.04% N, and 0.05 to 0.5% Mn, and, if required, containing one or more kinds selected from 0.1 to 2% Mo, 0.05 to 1.0% Fe, and 0.01 to 0.1% Si, and the balance Ni with inevitable impurities, and in which the content of C included as the inevitable impurities is controlled to 0.05%. PCOPYRIGHT: (C)2003,JPO
机译:

要解决的问题:提供一种镍基合金,该合金对因有机有害物质如PCB(多氯联苯)和二恶英的分解和氧化而引起的对含有盐酸等无机酸的超临界水具有优异的耐腐蚀性,并且提供用于由Ni基合金组成的超临界水处理反应容器的构件。

解决方案:对含无机酸的超临界水环境具有优异的耐腐蚀性的Ni基合金的成分为29至<42%Cr,> 1至3%Ta,0.001至0.05%Mg,0.001至0.04%N以及0.05至0.5%的Mn,并且如果需要,包含选自0.1至2%的Mo,0.05至1.0%的Fe和0.01至0.1%的Si中的一种或多种,​​余量的Ni具有不可避免的杂质,其中作为不可避免的杂质所包含的C的含量被控制为0.05%。

版权:(C)2003,日本特许厅

著录项

  • 公开/公告号JP4151062B2

    专利类型

  • 公开/公告日2008-09-17

    原文格式PDF

  • 申请/专利权人 三菱マテリアル株式会社;

    申请/专利号JP20020001218

  • 发明设计人 菅原 克生;

    申请日2002-01-08

  • 分类号C22C19/05;B01J3;B01J3/04;

  • 国家 JP

  • 入库时间 2022-08-21 20:21:17

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号