A multilayer, heat-shrinkable film has a first layer that is an outer film layer and that serves as a heat seal layer, and a second layer comprising at least one semi-crystalline polyamide. The first layer contains at least one member selected from the group consisting of (i) polyolefin having a density of from 0.88 g/cm3 to 0.917 g/cm3, and (ii) ionomer resin. The second layer contains at least one semi-crystalline polyamide selected from the group consisting of polyamide 6, polyamide 66, polyamide 6/66, and polyamide 6/12, with the semi-crystalline polyamide making up at least 50 weight percent of the second layer. The film has a total free shrink at 185° F. of at least 35 percent. The film has a total semi-crystalline polyamide content of at least 35 volume percent. The multilayer, heat-shrinkable film exhibits a percent haze as measured using ASTM D 1003-00, and a percent transparency as measured using ASTM D 1746-97, in accordance with the following equation: % Transparency≧5.33 (% Haze)−31.5 The multilayer, heat-shrinkable film can be used to make a packaging article.
机译:多层可热收缩膜具有第一层和第二层,该第一层是外膜层并用作热封层,第二层包含至少一种半结晶聚酰胺。第一层包含选自以下的至少一个:(i)密度为0.88 g / cm 3 至0.917 g / cm 3 的聚烯烃,和(ii)离聚物树脂。第二层包含至少一种选自聚酰胺6,聚酰胺66,聚酰胺6/66和聚酰胺6/12的半结晶聚酰胺,其中半结晶聚酰胺占第二层的至少50重量%。层。薄膜在185°F时的总自由收缩率至少为35%。该膜的总半结晶聚酰胺含量为至少35体积%。该多层可热收缩膜根据以下方程式显示出使用ASTM D 1003-00测量的雾度百分比和使用ASTM D 1746-97测量的透明度百分比:透明度百分比≥5.33(雾度百分比)-31.5多层可热收缩的膜可用于制造包装制品。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号