首页> 外国专利> 2. Concentration process of anatas mechanical concentrate for the purpose of obtaining synthetic ruby with low content of radioactive elements and rare earth elements

2. Concentration process of anatas mechanical concentrate for the purpose of obtaining synthetic ruby with low content of radioactive elements and rare earth elements

机译:2.为获得放射性元素和稀土元素含量低的合成红宝石而进行的anatas机械浓缩物的浓缩工艺

摘要

These include: (a) burning the anatasa concentrate between 400 and 600 ° C in 15 to 60 minutes, in which case the ferric oxide hydrate is converted to blood after pumping; (b) using H2, natural gas or any carbon reducing solid (metallurgical coke), reducing the burnt product from 400 to 600 ° C for 5 to 30 minutes in 5 to 30 minutes. 1. Carbonate, petroleum coke, graphite) convert mercury to magnesium; (c) use 600 to 800 Gauss magnetic field to separate the dry magnetic field or sparse magnetic field of the thin product, and remove (b) the magnetic component produced;(d) separation of dry or wet magnetic from low-density non-magnetic products with magnetic fields between 10000 and 15000 Gauss and extraction of silicates from silicates, diphosphates, monkeys, calcium, zirconium and minerals containing u and H; and 1. Dissolve 20-25% w / W HCl, 90-107 ℃ and 2-4 h, and extract impurities rich in faith, phosphate, Mg, Ba, Ka, sir, rare earth, u and th; (f) filtration and leaching products; (g) drying and filtration products; (H) oxidation and drying products 900-1200 ℃; (I) cooling products oxidized into compressed water or air;(J) leaching at 135 ° C with 25% w / W HCl or 55% w / W H2SO4 solution; (k) filtering the product; and (L) drying the filtered product by recovering the non-magnetic part such as rutile compound (final product);
机译:这些措施包括:(a)在15至60分钟内于400至600°C的温度下燃烧Anatasa浓缩液,在这种情况下,三氧化二铁水合物在泵送后转化为血液; (b)使用H2,天然气或任何减碳固体(冶金焦),在5至30分钟内将燃烧产物从400至600°C还原5至30分钟。 1.碳酸盐,石油焦,石墨)将汞转化为镁; (c)使用600至800高斯磁场来分离薄产品的干磁场或稀疏磁场,并去除(b)产生的磁性成分;(d)将干或湿磁与低密度非磁性物质分离。具有10000至15000高斯磁场的磁性产品,并从硅酸盐,二磷酸盐,猴子,钙,锆和含u和H的矿物中提取硅酸盐; 1.溶解20-25%w / W HCl,90-107℃和2-4 h,并提取富含信念的杂质,磷酸盐,Mg,Ba,Ka,先生,稀土,u和th。 (f)过滤和浸出产品; (g)干燥和过滤产品; (八)氧化干燥产物900-1200℃; (I)冷却产物氧化成压缩水或空气;(J)在135°C下用25%w / W HCl或55%w / W H2SO4溶液浸出; (k)过滤产品; (L)通过回收非磁性部分例如金红石化合物(最终产物)来干燥过滤产物;

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号