There are provided a steel for warm working, to be subjected to warm working as various structures, components of cars, and the like, a warm working method thereof, and a steel material and a steel component obtainable from the warm working method. [Solving Means] A steel is to have a particle dispersion type fiber structure formed in the matrix by warm working. The steel is characterized in that the total amount of the dispersed second-phase particles at room temperature is 7 × 10-3 or more in terms of volume fraction, and the Vickers hardness (HV) is equal to or larger than the hardness H of the following equation (2):H = (5.2 - 1.2 × 10-4λ) × 102 ... (2)when the steel is subjected to any of annealing, tempering, and aging treatments in the as-unworked state under conditions such that a parameter λ expressed by the following equation (1):λ = T(logt + 20) (T; temperature (K), t; time (hr)) ... (1)is 1.4 × 104 or more in a prescribed temperature range of 350°C or more and Ac1 point or less. This steel is taken as the steel for warm working.
机译:提供一种用于热加工的钢,该热加工的钢作为汽车的各种结构,部件等进行热加工,其热加工方法,以及可以从该热加工方法获得的钢材和钢部件。 [解决手段]钢应具有通过热加工在基体中形成的颗粒分散型纤维结构。该钢的特征在于,室温下分散的第二相粒子的总量以体积分数计为7×10-3以上,并且维氏硬度(HV)等于或大于H 2的硬度H。下式(2):高=(5.2-1.2×10-4λ)×102 ...(2)当在未经加工的状态下对钢进行任何退火,回火和时效处理的条件下,其条件λ由以下等式(1)表示:λ= T(logt + 20)(T;温度(K),t;时间(hr))...(1)在350℃以上且Ac1点以下的规定温度范围内,为1.4×104以上。该钢被用作热加工用钢。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号