Method For Asphalt Concrete Pavement and Method For Manufacturing Blocks Using Aggregates Reproduced From Waste Cement Concrete

机译:废水泥混凝土再生骨料的沥青混凝土路面施工方法和砌块制造方法

摘要

An asphalt concrete road pavement method and a block manufacturing method using reclaimed aggregates from waste asphalt concrete are provided to improve the durability of a pavement or a block by manufacturing asphalt concrete with reclaimed aggregates from waste cement concrete and to make a pavement or a block to have semi-rigidity by mixing the flexibility of asphalt and the stiffness of cement appropriately. An asphalt concrete road pavement method using reclaimed aggregates from waste asphalt concrete comprises the steps of: crushing waste asphalt concrete and sorting out aggregates in the appointed particle size distribution to have the wanted porosity; emulsifying asphalt attached on the surface of the reclaimed aggregates from waste asphalt concrete, mixing 0.01~0.10 weight percent emulsified asphalt of 1 weight percent reclaimed aggregates from waste cement concrete with 5~50 weight percent water-soluble latex of the emulsified aspha inputting 0.02~0.12 weight percent cement of 1 weight percent reclaimed aggregates from waste cement concrete and water to the mixed reclaimed aggregates, the emulsified asphalt and the latex, and mixing all together to make asphalt concrete to have 8~30 percent porosity and 0~3-centimeter slump value; and completing a paved road by carrying the produced asphalt concrete to a construction site, spreading and tamping with a roller, or, completing a block having a thickness of 60 cm by inputting the produced asphalt concrete in a mold, vibrating, pressurizing and curing.
机译:提供了一种沥青混凝土路面的铺装方法和使用废沥青混凝土的再生骨料的砌块制造方法,以通过利用废水泥混凝土的再生骨料制造沥青混凝土并制造路面或砌块来提高路面或砌块的耐久性。通过适当地混合沥青的柔韧性和水泥的硬度而具有半刚性。一种使用废沥青混凝土中的再生骨料的沥青混凝土路面方法,包括以下步骤:压碎废沥青混凝土,并按照指定的粒度分布将骨料分类以具有所需的孔隙度;将乳化沥青附着在废沥青混凝土的再生骨料表面上,将0.01〜0.10重量%的乳化沥青和1重量%的废水泥混凝土的再生骨料与5〜50重量%的乳化沥青的水溶性胶乳混合;将废水泥混凝土和水中的1重量%的再生骨料的0.02〜0.12重量%的水泥输入到混合的再生骨料,乳化沥青和乳胶中,并混合在一起,使沥青混凝土的孔隙度为8%至30%,0% 3厘米的坍落度值;通过将生产的沥青混凝土运送到施工现场,用辊子摊开和夯实来完成铺路,或者通过将生产的沥青混凝土输入到模具中,振动,加压和固化来完成厚度为60厘米的砌块。

著录项

  • 公开/公告号KR100788050B1

    专利类型

  • 公开/公告日2007-12-24

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20060125380

  • 发明设计人 황익현;

    申请日2006-12-11

  • 分类号E01C7;C04B18/16;E01C5;

  • 国家 KR