首页> 外国专利> CONSTRUCTION PLANK OF IMITATION STONE AND ITS MAKING METHOD USING FELDSPAR

CONSTRUCTION PLANK OF IMITATION STONE AND ITS MAKING METHOD USING FELDSPAR

机译:仿石的施工平板及其制作方法

摘要

A method for manufacturing an artificial stone board for building is provided to produce the artificial stone board that emits far infrared rays and anions, has increased bonding strength, and displays various color tones. A method for manufacturing artificial stone boards for building comprising 50-70wt.%of feldspar as a main material includes the steps of: charging 30-60wt.%of feldspar powder having a particle size of about 1-4 mm, 10-20wt.%of feldspar aggregate having a particle size of about 5-10 mm, 8-15wt.%of red elvan having a particle size of about 4-8 mm, 7-15wt.%of germanium ore powder having a particle size of 20 mesh and smaller, and 15-20wt.%of an inorganic solidifying agent having a particle size of about 4-8 mm into a mixer, and mixing the materials to obtain a mixture; charging 5-10wt%, based on the total weight of the mixture, of water into the mixer, mixing and kneading the admixture evenly, and applying more than 600 ton of force to a mold containing the kneaded material to obtain a molded artificial stone board; drying the molded artificial stone board in the shade having a temperature of 15-20 °C for about 2-4 days after demolding; and polishing the artificial stone board using an electric grinder. Further, the inorganic solidifying agent is selected from shellfish solidifying agent, eco cement, meta kaolin, white cement or high strength cement.
机译:提供一种用于制造建筑用人造石板的方法,以生产发出远红外线和阴离子,具有增加的结合强度并显示各种色调的人造石板。一种用于制造以50-70重量%的长石作为主要材料的建筑用人造石板的方法,包括以下步骤:装料粒度为约1-4mm,10-20wt%的30-60重量%的长石粉末。 %的长石聚集体,其粒度为约5-10mm,8-15wt。%的红色elvan,其粒度为约4-8mm,7-15wt。%,为粒度为20目的锗矿粉将较小的无机固化剂和15-20wt。%的粒径为约4-8mm的无机固化剂放入混合器中,并将这些材料混合以获得混合物;将基于混合物总重量的5-10wt%的水倒入混合器中,将混合物均匀地混合和捏合,并向装有捏合材料的模具施加600吨以上的力,以获得人造石板成型体;脱模后,将成型的人造石板在温度为15-20℃的阴凉处干燥约2-4天;并用电动磨床抛光人造石板。此外,无机固化剂选自贝类固化剂,生态水泥,间高岭土,白水泥或高强度水泥。

著录项

  • 公开/公告号KR100791526B1

    专利类型

  • 公开/公告日2008-01-09

    原文格式PDF

  • 申请/专利权人 CHUNG WOO INDUSTRIAL CO. LTD.;

    申请/专利号KR20070045592

  • 发明设计人 CHA WHA SIN;

    申请日2007-05-10

  • 分类号C04B14/02;B28B3;C04B28;

  • 国家 KR

  • 入库时间 2022-08-21 19:52:42

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号