首页> 外国专利> Process for preparing 4A type zeolite

Process for preparing 4A type zeolite

机译:制备4a型沸石的方法

摘要

This invention relates to a method of producing a high degree of whiteness is 4A type zeolite, more specifically, aluminum mixing aluminum dross and sodium hydroxide solution by-product in the refining process at a specific ratio and, by itself, the reaction conditions at a temperature and pressure conditions generated in the reaction mixture, such as coloring components, unlike the conventional method and made from high temperature and high pressure spilling can extract the sodium aluminate is not substantially contain impurities into the aqueous phase, this aqueous solution of sodium silicate and hydro gel to the reaction, aging (ageing) by hydrothermal synthesis reaction and at the same time producing the excellent whiteness purity over the course of the zeolite There will still be available, as well as circulation of the mother liquor Improvement of the production cost savings and environmentally friendly method of producing an improved effect on 4A zeolite having at the same time.
机译:本发明涉及一种高白度的4A型沸石的生产方法,更具体地讲,涉及一种铝,其在精制过程中以特定比例混合铝渣和氢氧化钠溶液副产物而制得,其自身的反应条件为在反应混合物中产生的温度和压力条件下,例如着色组分,与常规方法不同,并且由高温和高压溢出制成,可以萃取出基本上不含杂质的铝酸钠进入水相,这种硅酸钠水溶液和将水凝胶加入反应中,通过水热合成反应进行老化(老化),同时在沸石过程中产生优异的白度纯度。母液的循环以及循环仍可使用。节省生产成本同时对4A沸石产生改善效果的环保方法。

著录项

  • 公开/公告号KR100831758B1

    专利类型

  • 公开/公告日2008-05-23

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20040041049

  • 发明设计人 서정권;이정민;

    申请日2004-06-04

  • 分类号C01B39/14;B01J29/06;

  • 国家 KR

  • 入库时间 2022-08-21 19:52:03