An environment-friendly bamboo floor material manufacturing method and bamboo floor materials produced by using the same are provided to use the bamboo floor materials for a long time by preventing cracks and a joint from being gaped. An environment-friendly bamboo floor material manufacturing method comprises the steps of: removing moisture by placing extracted bamboos in the shade for 60 days; forming bamboo members(111) by cutting the bamboos into plural parts with keeping the predetermined standard; boiling the cut bamboo members at 100°C for 4 hours by sinking the bamboo members in the solution containing germanium and phytoncide mixed in the certain quantity of water; forcibly drying the boiled bamboo members by exposing the bamboo members to the sunlight for 7 days; drying the forcibly dried bamboo members at high temperature in a closed space of 300°C; exposing the bamboo members dried at high temperature, to the wind of 10~20m/sec. for 36 hours; shearing the surfaces of the bamboo members; bonding the bamboo members in many folds by applying a natural vegetable adhesive at the edge of the bamboo members; compressing the bamboo members by applying compression strength of 600~800kg/cm^2; forming bamboo panels(110) by cutting the compressed bamboo members in the predetermined size; forming an air suction unit at the bottom side of the cut bamboo panels in a longitudinal direction; treating the bamboo panels having the air suction units at high temperature by applying heat increased at an interval of 1 hour for 5 hours; stacking the bamboo panels in order and naturally drying the stacked bamboo panels for 7 days; and polishing the surfaces of the naturally dried bamboo panels by using a pulp non-woven fabric.
机译:提供一种环保的竹地板材料的制造方法和使用该方法制造的竹地板材料,以通过防止裂缝和接缝开裂而长时间使用该竹地板材料。一种环保的竹地板材料的制造方法包括以下步骤:通过将提取的竹子放在阴凉处60天以除去水分;通过在保持预定标准的情况下将竹子切割成多个部分而形成竹子构件(111);将切好的竹子浸入混有一定量的水的锗和植物杀菌剂的溶液中,在100℃下煮沸4小时。将煮过的竹子暴露在阳光下7天,强行烘干。将被强力干燥的竹构件在300°C的密闭空间中高温干燥;暴露在高温下干燥的竹子构件,风速为10〜20m / sec。 36小时;剪竹构件的表面;通过在竹构件的边缘上涂天然植物粘合剂,将竹构件折成许多折。通过施加600〜800kg / cm ^ 2的压缩强度来压缩竹构件。通过将压缩的竹构件切割成预定尺寸来形成竹板(110);在切下的竹板的底侧沿纵向形成吸气单元。以1小时为间隔,每隔5小时加热一次,对具有吸气单元的竹板进行高温处理。依次堆叠竹板,自然干燥堆叠的竹板7天;使用纸浆无纺布对天然干燥的竹板的表面进行抛光。

著录项

  • 公开/公告号KR100847004B1

    专利类型

  • 公开/公告日2008-07-21

    原文格式PDF

  • 申请/专利权人 HUDIGM ARCHITECTS & ENGINEERS CO. LTD.;

    申请/专利号KR20070133357

  • 发明设计人 KIM HWANG PYUNG;

    申请日2007-12-18

  • 分类号B27J1/00;B27J1/02;

  • 国家 KR

  • 入库时间 2022-08-21 19:51:49

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号