A porous artificial fish reef is provided to foster plankton in marine environment, to prevent the oxidation of the fish reef and to form better fishing ground by employing electro arc furnace oxidizing slag in the artificial fish reef. A porous artificial fish reef is prepared by a process comprising: mixing water of 100-150kg/m^3, cement of 290-380kg/m^3, aggregate having size of 13-2.5mm of 1590-1950kg/m^3, high strength admixture of 30-120kg/m^3, CSA expander of 3-4kg/m^3, pigment of 10-40kg/m^3 and at most 0.3% of retardant; molding the mixture in a mold; and curing the mixture. The aggregate is the electro arc furnace oxidizing slag which is generated from a steelmaking process using pig iron in electro arc furnace. The mold has a form of a cube. For the curing, the mixture is subjected to an open stowage for 28 days or subjected to a steam chamber.
展开▼
机译:通过在人造鱼礁中使用电弧炉氧化炉渣,提供了多孔的人造鱼礁来在海洋环境中培育浮游生物,以防止鱼礁的氧化并形成更好的渔场。通过以下方法制备多孔人工鱼礁,该方法包括:混合100-150kg / m ^ 3的水,290-380kg / m ^ 3的水泥,13-2.5mm的骨料1590-1950kg / m ^ 3, 30-120kg / m ^ 3的高强度混合物,CSA膨胀剂3-4kg / m ^ 3,颜料10-40kg / m ^ 3和最多0.3%的阻燃剂;将混合物在模具中模制;并固化混合物。骨料是电弧炉氧化渣,它是在电弧炉中使用生铁从炼钢过程中产生的。模具具有立方体的形式。为了固化,将混合物进行开放式存放28天或置于蒸汽室中。
展开▼