首页> 外国专利> METHOD FOR PRODUCING permanent magnets NEODYMIUM Alloys (praseodymium)-iron-boron

METHOD FOR PRODUCING permanent magnets NEODYMIUM Alloys (praseodymium)-iron-boron

机译:永久磁铁钕合金(pr)-铁硼的生产方法

摘要

1. A method for producing permanent magnets of alloys based systems neodymium-iron-boron, praseodymium-iron-boron comprising molding the preform and subsequent hot deformation, characterized in that the deformation is performed by equal-channel angular extrusion at intersecting vertical and horizontal channels crossing angle equal to 90-135 ° in the temperature range 500-800 ° C, to achieve a logarithmic cumulative degree of deformation of at least 0,5.2. A method according to claim 1, characterized in that after equal channel angular extrusion carry additional single-stage or multi-stage annealing at temperatures of 500-1000 ° C.3. A method according to claim 1, characterized in that after equal channel angular extrusion operations carried out additional hot deformation preform precipitation methods, rolling, extrusion at a temperature of 500-1000 ° C.4. A method according to claim 3, characterized in that the following further hot deformation operations carried out single-stage or multi-stage annealing at a temperature of 500-1000 ° C.
机译:1.一种用于生产基于合金的系统的钕铁硼,ase铁硼的永磁体的方法,其包括模制预型件并随后进行热变形,其特征在于,变形是通过在垂直和水平相交处的等通道角挤压而进行的。在500-800°C的温度范围内,通道的交叉角等于90-135°,以达到至少0.5.2的对数累积变形度。 2.根据权利要求1所述的方法,其特征在于,在等通道角挤压之后,在500-1000℃的温度下进行另外的单级或多级退火。 2.根据权利要求1所述的方法,其特征在于,在相等通道的角挤压操作之后,进行了另外的热变形预成型坯沉淀方法,在500-1000℃的温度下轧制,挤压4。 4.根据权利要求3所述的方法,其特征在于,以下进一步的热变形操作在500-1000℃的温度下进行了单阶段或多阶段退火。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号