A method of preparing a bitumen/polymer composition resistant to petroleum solvents involves contacting at 100-230 degreesC for 10 minutes or more a bitumen and, with respect to it, 0.3-20 wt.% of a crosslinkable elastomer, 0.05-15 wt.% of a functionalized olefin polymer of specified composition and a sufficient of a coupling agent to produce free sulfur representing 0.1-20 wt.% of the weight of the crosslinkable elastomer. The olefin polymer comprises: x wt.% of units deriving from ethylene or propylene, y wt.% of units deriving from one or more monomers of Formula: CH2=CR1R2 R1 = H, -CH3, -C2H5; R2 = -COOR5, -OR5, -OOCR6; R5 = 1-10C alkyl; R6 = H, 1-3C alkyl, and z wt.% of unit deriving from one or more monomers of Formula: R3-CH=CR1R4 R3 = H, -COOH, COOR5; R3 = -COOH, -OH, -COO-CH2-CH(O)CH3, -O- CH2-CH(O)CH2 x is greater than y+10 and greater than z, which is 0-20. An INDEPENDENT CL AIM is included for a bitumen/polymer composition produced by the above method
机译:制备抗石油溶剂的沥青/聚合物组合物的方法包括在100-230℃下接触沥青10分钟或更长时间,并且相对于其,0.3-20wt。%的可交联弹性体,0.05-15wt。%。 %的特定组成的官能化烯烃聚合物和足以产生游离硫的偶联剂,所述游离硫占可交联弹性体重量的0.1-20wt%。所述烯烃聚合物包含:xwt。%的源自乙烯或丙烯的单元,ywt。%的源自一种或多种式:CH 2 = CR 1 R 2 R 1 = H,-CH 3,-C 2 H 5的单体的单元; R2 = -COOR5,-OR5,-OOCR6; R5 = 1-10C烷基; R6 = H,1-3C烷基和z重量%的单元,其衍生自一种或多种下式的单体:R3-CH = CR1R4 R3 = H,-COOH,COOR5;和R 3 = -COOH,-OH,-COO-CH 2 -CH(O)CH 3,-O-CH 2 -CH(O)CH 2 x大于y + 10且大于z,其为0-20。通过上述方法生产的沥青/聚合物组合物包含独立的CL AIM

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号