首页> 外国专利> Preparing bituminous product and aggregate mixture, useful for preparing materials e.g. in the field of sealing, construction and road carpet maintenance and pavements, comprises mixing the product with the aggregate containing an additive

Preparing bituminous product and aggregate mixture, useful for preparing materials e.g. in the field of sealing, construction and road carpet maintenance and pavements, comprises mixing the product with the aggregate containing an additive

机译:制备沥青产品和骨料混合物,可用于制备例如在密封,建筑,道路地毯的维护和铺装领域,包括将产品与含有添加剂的骨料混合

摘要

Process for preparing bituminous product and aggregate mixture comprises mixing the product with the aggregate containing at least an additive (A), where: the mixing is carried out with temperature granular fractions, for producing a coating at a temperature of 60-200, preferably 100-200[deg] C; the temperature for producing aggregate and bituminous product mixture in production outlet is lowered up to 50?C; and the temperature of the aggregates and bituminous product mixture during spreading is lowered to 5-50[deg] C. Process for preparing bituminous product and aggregate mixture comprises mixing the product with the aggregate containing at least an additive of formula ((R-O-(CH 2CH(CH 3)O) a-(CH 2CH 2O) b) cP(=O)-OH d) (A), where: the mixing is carried out with temperature granular fractions, for producing a coating at a temperature of 60-200, preferably 100-200[deg] C; the temperature for producing aggregate and bituminous product mixture in production outlet is lowered up to 50?C; the temperature of the aggregates and bituminous product mixture during spreading is lowered to 5-50[deg] C; the temperature of the aggregate and bituminous product mixture in core of the carpet at the beginning of compaction is lowered to 10-50[deg] C; and the dosage of (A) measured to the ton of bituminous product is 0.3-20 kg. P : phosphorus atom; either c : 1-2; or c+d : 3; a : 0-80; b : 0-10; and R : 6-30C hydrocarbon chain (optionally saturated and optionally contain an aromatic core, structure of polypropylene glycol parts and polyethylene glycol optionally statistical or in blocks, the order of blocks is not restricted).
机译:制备沥青产品和骨料混合物的方法包括将产物与至少包含添加剂(A)的骨料混合,其中:混合是用温度颗粒级分进行的,以在60-200,优选100-200℃的温度下产生涂层。 -200℃;在生产出口处生产骨料和沥青产品混合物的温度降低到50℃。并且将铺展期间骨料和沥青产品混合物的温度降低至5-50℃。制备沥青产品和骨料混合物的方法包括将产品与至少包含式((RO-( CH 2CH(CH 3)O)a-(CH 2CH 2O)b)cP(= O)-OH d)(A)其中:与温度粒状组分进行混合,以在60-200,优选100-200℃;在生产出口处生产骨料和沥青产品混合物的温度降低到50℃。在铺展过程中,骨料和沥青产品混合物的温度降低到5-50℃。在压实开始时,地毯芯中的骨料和沥青产品混合物的温度降低到10-50℃; (A)相对于每吨沥青产品测得的剂量为0.3-20 kg。 P:磷原子;要么c:1-2;或c + d:3; a:0-80; b:0-10; R:6-30C烃链(任选地饱和并且任选地包含芳族核,聚丙二醇部分和聚乙二醇的结构任选地统计或成块,对嵌段的顺序没有限制)。

著录项

  • 公开/公告号FR2915485A1

    专利类型

  • 公开/公告日2008-10-31

    原文格式PDF

  • 申请/专利权人 CECA SA SOCIETE ANONYME;

    申请/专利号FR20070054724

  • 发明设计人 BARRETO GILLES;GRAMPRE LIONEL;

    申请日2007-04-26

  • 分类号C08L95;C08K5/521;C09D195;E01C7/22;E04B1/66;

  • 国家 FR